09CrCuSb ND Seamless Pipe

09CrCuSb ND Seamless Pipe

A low-alloy ND steel 09CrCuSb resistant to the dew-point corrosion of sulfuric acid for seamless steel pipe, plate, forged part and special welding material is prepared through smelting in ultra high-power electric furnace, refining outside the furnace, vacuum degassing, conticasting and tandem rolling.
Send Inquiry
Description
Technical Parameters

Product Description

 

09CrCuSb (ND Steel) Low-alloy Steel Tube for sulfuric acid proof dew point corrosive

A low-alloy ND steel 09CrCuSb resistant to the dew-point corrosion of sulfuric acid for seamless steel pipe, plate, forged part and special welding material is prepared through smelting in ultra high-power electric furnace, refining outside the furnace, vacuum degassing, conticasting and tandem rolling.

It features that during the corrosion, a compact passivated film rich in Cr, Cu, Sb and Ti is generated on its surface, so having very high anticorrosion power.

ND steel is a low-alloy structural steel. Compared with other steel types such as low-carbon steel, Corten, CR1A, etc., ND steel has excellent corrosion resistance and mechanical properties.

image001

 

Specifications

 

Pipe Standard

GB 3087, GB 5310

O.D

12.7mm - 127mm

W.T

0.9 - 12.7mm

Grade

09CrCuSb

Process

Hot Finished or Cold Finished

Heat Treatment

Normalized or as per request

Tests

Tension, flattening, flaring, flange, hardness, reverse flattening, and hydrostatic tests

Application

Pressure containing parts, Economizer, APH (Air Preheater) and other corrosion-resistant applications.

 

Material standards

 

① GB 150.2-2011 "Pressure Vessel Part 2: Materials"

② NB/T 47019-2011 "Technical conditions for ordering boiler and heat exchanger tubes"

③ SH/T 3096-2012 "Principle of Material Selection for High Sulfur Crude Oil Processing Equipment and Pipeline Design"

 

Mechanical Property

 

Nominal Thickness

(mm)

Tensile Strength

Rm (MPa)

Yield Strength

ReL (MPa)

Elongation

A (%)

≤8

390~550

≥245

≥25

 

Product Detail

 

image003
image005
image007
image009

 

Corrosion resistance

 

In sulfuric acid of medium-temperature and medium concentration, ND steel is passivated due to dissolution, and a passivation layer rich in alloy elements such as Cu, Cr, Sb (antimony, sound: tī) is formed on the surface of the steel and has a high Sulfuric acid corrosion resistance.

 

Corrosion rate comparison between ND steel and other steels

 

Type of Steel

Corrosion Rate

mg/(cm2h)

Times

ND (09CrCuSb)

7.3

1

A3 (Q235B)

103.5

14.18

CORTEN-A

63

8.63

CR1A

13.4

1.84

321

21.7

2.97

S-TEN 1 & 2

27.4

3.75

For the corrosion resistance, GB 150.2-2011 stipulates: The steel pipe shall be tested for corrosion resistance, and one sample shall be taken from each of the two steel pipes in each batch, and each sample shall be a pipe length of 10 mm.

Soak in a H2SO4 solution with a mass fraction of 50% at a constant temperature of 70°C (±2°C) for 24 hours. The average value of the corrosion rate of the two samples is not greater than 80g/m2×h or 140g/m2×h, the specific indicators are indicated in the order contract.

 

Application

 

ND steel is currently the most ideal steel for "sulfuric acid low-temperature dew point corrosion resistance" at home and abroad, and its seamless steel tubes are widely used in the manufacture of economizers, air preheaters, heat exchangers and evaporations that are used in high sulfur flue gas The device and other equipment are used to resist the dew point corrosion of sulfur-containing flue gas.

image011

 

FAQ

 

Q: How is the delivery time?

A: It depends your order quantity.

Q: How do you control the quality?

A: We have QC team comply with TQM to ensure the quality. Each step is in compliance to the standards. At the same time, we will take photos and shoot video for you if you need. Every product will be fully assembled and carefully tested before packing and shipping.

Q: How to buy it? What about the delivery?

A: Please contact me by email or online, let me know your situation, I will give you professional solution. We have shipping agent can choosing the cheapest and fastest delivery. FOB, CIF, C&F or EXW are no problem for us.

 

Hot Tags: 09crcusb nd seamless pipe, China 09crcusb nd seamless pipe manufacturers, suppliers, Round corten Pipe, corten pipe, Round Corten Steel Pipe, weathering steel pipe, Square Corten Steel Tube, corten steel tube