Pre-rusted Corten Plate refers to weathering steel that has undergone an accelerated oxidation process through artificial treatment. This process allows the steel surface to develop a stable and uniform rust-like patina within a short period of time, achieving the visual effect of natural weathering that would normally take months or even years.
Send Inquiry
Description
Technical Parameters

Product Description

 

Pre-rusted Corten Plate refers to weathering steel that has undergone an accelerated oxidation process through artificial treatment.

This process allows the steel surface to develop a stable and uniform rust-like patina within a short period of time, achieving the visual effect of natural weathering that would normally take months or even years.

Compared to untreated weathering steel that relies on natural exposure to form a patina, pre-rusted Corten plates offer a more consistent color tone and denser oxide layer. This not only provides a refined and visually appealing surface, but also ensures more stable corrosion resistance in long-term use.

Pre-rusted Corten steel plates are widely used in projects where aesthetic quality and surface texture are essential, such as architectural facades, landscape design, urban public art installations, outdoor sculptures, commercial exteriors, and interior industrial-style decor. The distinctive rusted texture pairs harmoniously with natural materials like wood, stone, and greenery, creating strong visual impact and an artistic atmosphere.

image001

 

Specifications

 

Thickness

Dimensions (mm / inches)

Weight (kg)

1.5mm / 16SWG (0.059 in)

400mm × 200mm (approx. 16 in × 8 in)

0.94kg

1.5mm / 16SWG (0.059 in)

500mm × 500mm (approx. 20 in × 20 in)

2.9kg

1.5mm / 16SWG (0.059 in)

600mm × 300mm (approx. 24 in × 12 in)

2.12kg

1.5mm / 16SWG (0.059 in)

750mm × 750mm (approx. 30 in × 30 in)

6.6kg

1.5mm / 16SWG (0.059 in)

900mm × 600mm (approx. 36 in × 24 in)

6.36kg

1.5mm / 16SWG (0.059 in)

1000mm × 1000mm (approx. 40 in × 40 in)

12kg

1.5mm / 16SWG (0.059 in)

1250mm × 1000mm (approx. 50 in × 40 in)

15kg

1.5mm / 16SWG (0.059 in)

1250mm × 1250mm (approx. 50 in × 50 in)

18kg

1.5mm / 16SWG (0.059 in)

1500mm × 1000mm (approx. 60 in × 40 in)

18kg

1.5mm / 16SWG (0.059 in)

2000mm × 1000mm (approx. 80 in × 40 in)

24kg

1.5mm / 16SWG (0.059 in)

2500mm × 1250mm (approx. 100 in × 50 in)

37kg

 

Product Pictures

 

image003
image005
image007
image009

 

Applications

 

image011

 

Pre-rusted Corten Plate is widely used in both architectural and landscape applications due to its distinctive rusted finish and excellent weather resistance. It is ideal for building façades, exterior wall cladding, and decorative panels, offering a natural, aged look that enhances modern and industrial design aesthetics. In landscape and urban design, it is commonly used for planter boxes, retaining walls, edging, and street furniture.

 

The plate is also perfect for outdoor sculptures and public art installations, requiring no painting or maintenance. In infrastructure projects, it is used for bridges, noise barriers, signage, and shelters. Indoors, it can be applied to feature walls, partitions, ceilings, and stair elements, creating a bold and textured visual effect. Its strong weathering performance also makes it suitable for industrial enclosures and equipment covers exposed to harsh environments.

image013

Hot Tags: pre-rusted corten plate, China pre-rusted corten plate manufacturers, suppliers, High durability steel coil, Corten B, 09CrCuSb Corten Plate, Corten Steel for Acid Dew Resistance, Perforated Corten Steel, weathering steel sheet