High Quality 09CuPTiRE-B Corten Steel Plate

High Quality 09CuPTiRE-B Corten Steel Plate

09CuPTiRE-B steel plate is a low-alloy weathering structural steel specifically formulated with copper, chromium, nickel, and phosphorus. This composition not only enhances the plate's atmospheric corrosion resistance but also provides superior resistance to flue gas and high-humidity environments. Simultaneously, it promotes the formation of a stable oxide layer on the surface, yielding a distinctive color and aesthetic appeal.
Send Inquiry
Description
Technical Parameters

Products Description

 

09CuPTiRE-B Weather Resistant Steel PlateHigh Quality 09CuPTiRE-B Corten Steel Plate is a low-alloy weathering structural steel specifically formulated with copper, chromium, nickel, and phosphorus.

 

This composition not only enhances the plate's atmospheric corrosion resistance but also provides superior resistance to flue gas and high-humidity environments.

 

Simultaneously, it promotes the formation of a stable oxide layer on the surface, yielding a distinctive color and aesthetic appeal.

 

In terms of performance, 09CuPTiRE-B Weathering Steel Plate typically exhibits a yield strength of no less than 345 MPa (for thickness ≤16 mm), tensile strength ranging from 470–630 MPa, elongation ≥20%, and impact energy exceeding 27 J at -20°C.

 

These metrics ensure the steel plate's reliability under prolonged loading and harsh climatic conditions.

 

Leveraging its combination of mechanical strength and corrosion resistance, 09CuPTiRE-B corten steel plate finds extensive application in vehicle manufacturing, bridge construction, transmission tower structures, containers, and chemical vessels.

 

In practical use, its service life can be 4–8 times longer than ordinary carbon steel, with significantly reduced maintenance costs. Consequently, it offers high economic value and practicality in engineering projects.

 

09CuPTiRE-B Weathering steel plate chemcial composiiton

 

Grade

C

Si

Mn

P

09CuPTiRE-B

≤0.12

0.20-0.50

0.25-0.7

0.06-0.12

S

RE

Cu

Ti

≤0.020

0.01-0.04

0.25-0.50

≤0.030

 

09CuPTiRE-B Corten steel plate mechanical properties

 

Grade

Thickness mm

Yield strength min

Tensile strength min

Elongation % min

09CuPTiRE-B

-

345 Mpa

480 Mpa

24

 

09CuPTiRE-B weathering structural steel plate rolling size

 

Thickness

1.2-150mm

Width

1220-4200mm

Length

5000-18000

 

TB/T 1979 09CuPTiRE-B Weather Resistant Steel Sheet Application

 

TB/T 1979 09CuPTiRE-B weather resistant steel coil has wide applications such as Vehicle, Bridge, Tower and Containers.

 

Additional Condition

 

UT(Ultrasonic examination), AR(As Hot Rolled only), TMCP(Thermal Mechanical Control Processing), N(Normalized), Q+T(Quenched and Tempered),Z Direction Test(Z15,Z25,Z35), Charpy V-Notch Impact Test, The Third Party Test (such as SGS Test), Coated or Shot Blasting and Painting.

09CuPTiRE-B Weather Resistant Steel Sheet

 

Other Terms

 

Packaging Details: Standard export seaworthy packing or as required.


Delivery Time: 30-50 days, 7 days for stock goods.


Loading Port: Shanghai ,Tianjin, Qingdao.


Offer Ability: 5 000MT/Per Month.


MOQ: 1 Pcs.

 

Contact now to get 09CuPTiRE-B Quote

 

About Us

 

With robust R&D strength and flexible manufacturing systems, Gnee offers comprehensive OEM (Original Equipment Manufacturing) and ODM (Original Design Manufacturing) services to meet the diverse needs of global clients.

Our Services Include:

 

 OEM Manufacturing – Mass production of weathering steel products under your brand with quality assurance.

 

 ODM Design & Customization – Tailored services such as structural design, size customization, laser cutting, and surface treatment.

 

 Rapid Prototyping – Quick sample development based on drawings or creative sketches to meet tight project timelines.

 

Whether you're a brand owner, designer, or contractor, Gnee is your reliable partner for high-quality, custom steel solutions.

Corten Gnee

Hot Tags: high quality 09cuptire-b corten steel plate, China high quality 09cuptire-b corten steel plate manufacturers, suppliers, Pre rusted Corten Plate, corten plate, ASTM Weathering Steel Plate, corten steel coil, Hot rolled Corten A coil, perforated corten steel facade