Will the surface patina of Q355NH weathering steel screens become darker over time?

Mar 30, 2026 Leave a message

The surface patina of Q355NH weathering steel screens will indeed become darker over time, and it follows a clear color evolution rule.

 

Brief color change process

Early stage (0–1 year)

Bright orange‑red → reddish‑brown, loose rust layer, color relatively light.

Middle stage (1–3 years)

Gradually turns deep brown / chocolate brown, patina becomes dense, color obviously darkens.

Stable stage (3–5 years +)

Becomes dark brown to grayish‑brown, basically no longer bright red;In industrial or humid environments, it may even appear brown‑black.

info-457-441

Why it keeps darkening

1. Alloy elements (Cu, Cr, Ni, P) continuously enrich in the inner rust layer.

2. The oxide structure becomes denser and less light‑reflective.

3. Long‑term UV, humidity and atmospheric corrosion promote further oxidation.

info-470-448

How to stop darkening

If you want to fix the color at a certain brown tone and not let it get darker:

1. Wait until it reaches your desired shade

2. Spray a layer of matte transparent protective oil / clear coat to isolate air and moisture.

info-500-497