ASTM A847 Corten Steel Tube

ASTM A847 Corten Steel Tube

Standards:ASTM A 847 / ASME SA 847 Shape:round, square,rectangular, Hydraulic, Honed Tubes Squares Size :3″ through 12″ Rectangles Size:4″ x 2″ through 16″ x 8″ Rounds Size:6.625″OD, 8.625″OD, 10.75″OD, 12.75″OD, 14″OD and 16"OD Walls Thickness:125″ through .625″ Length:Single Random, Double Random & Cut Length Type:Weathering Steel End :Plain End, Beveled End
Send Inquiry
Description
Technical Parameters

Products Description

 

ASTM A 847

ASTM A847 Steel Pipe is a weathering steel that is a high-strength, low-alloy steel covering cold-formed welded square and rectangular tubing and pipe.

 

The atmospheric corrosion resistance of this steel is significantly better than that of carbon steel with or without added copper in most environments.

 

High Strength ASTM A847 Rectangular Tubing is intended for welded, bolted, or riveted construction of bridges and other structures where high strength and enhanced corrosion resistance are required.

 

ASTM A847 Corten Steel Tubes has a 50ksi minimum yield strength and a 70ksi minimum tensile strength.

 

Products specification

 

Standards:ASTM A 847ASTM A 847


Shape:round, square,rectangular, Hydraulic, Honed Tubes


Squares Size :3″ through 12″


Rectangles Size:4″ x 2″ through 16″ x 8″


Rounds Size:6.625″OD, 8.625″OD, 10.75″OD, 12.75″OD, 14″OD and 16"OD


Walls Thickness:125″ through .625″


Length:Single Random, Double Random & Cut Length


Type:Weathering Steel


End :Plain End, Beveled End

 

ASTM A847 Corten Steel Tube Chemical Composition

 

Elements Heat Analysis Product Analysis
Carbon Max 0.20 0.24
Manganese Max 1.35 1.40
Phosphorus Max 0.15 n/a
Sulpher Max 0.05 0.06
Copper Min 0.20 0.18

 

CORTEN A847 Weathering Steel Tube Mechanical Properties

 

Grade Yield Strength Min PSI Tensile Strength Min PSI Elongation % (min)
ASTM A847 50,000 70,000 19

 

ASTM A847 Corten Steel Pipe Applications

 

ASTM A847 Corten Steel Tube

• Pedestrian Bridges


• Highway Bridges


• Outdoor pavilions


• Architectural exposed structural applications


• Fencing


• Guardrail


• Guide Rail


• Sign Posts

 

 

ASTM A847 Corten Steel Tube is produced utilizing the best nature of materials and trend-setting innovation.

 

ASTM A847 Corten Weathering Steel Tube has some excellent features to offer such as a skilled workforce, quality resources used, executed within the assured time frame, and more.

 

Also, ASTM A847 Corten Steel Piping is recommended to use a high-temperature underlayment.