Products Description
Corten Steel B Pipes is highly favored by architects due to its ability to adapt to changing climatic conditions and natural landscapes, displaying an ever-evolving rustic patina on its surface.
Under normal atmospheric conditions, Corten B steel tubig develops a stable protective oxide layer, offering 4–8 times higher corrosion resistance compared to ordinary carbon steel, and typically eliminating the need for repainting or additional maintenance for 30–50 years.
With a tensile strength of around 485 MPa and a yield strength of approximately 345 MPa, it combines both strength and long-term durability.
When integrated with urban infrastructure, it delivers a striking finish that gives buildings a modern and stylish appearance. We provide our valued customers with Corten B steel tubes at highly competitive prices.
As Corten B steel piping grew in popularity, other steel mills also began producing their own atmospheric corrosion-resistant weathering steels.
Chemical Composition
| Size Range | ½ OD to 16 OD |
|---|---|
| Standards | ASTM A 423 GR. 1,ASME SA 423, ASTM A 847, ASTM 588, ASTM 606 |
| Grade | Corten B |
| Shape | Round, Square, Rectangle, Hydraulic, Honed Tubes |
| Length | Single Random, Double Random & Cut Length |
| End | Plain End, Beveled End |
| type | Weathering steel / corten steel |
Chemical Composition For Corten B Steel Pipes & Tubes
| Grade | C | Si | Mn | P | S | Cr | Cu | V | Ni |
|---|---|---|---|---|---|---|---|---|---|
| CORTEN B | 0.16 | 0.30–0.50 | 0.80–1.25 | 0.030 | 0.030 | 0.40–0.65 | 0.25–0.40 | 0.02–0.10 | 0.40 |
Mechanical Properties For Corten Steel B Pipes & Tubes
| Grade | Yield Strength MPa(min) |
Tensile Strength MPa |
Elongation % (min) |
|---|---|---|---|
| CORTEN B | 345 | 485 | 19 |
Corten Steel B Pipes & Tubes Equivalent Standard
| APPLICATION | BRITISH STANDARD | JAPANESEJIS | GERMAN DIN |
AMERICAN ASTM |
|---|---|---|---|---|
| AIR PRE HEATERS | BS-6323-5 BS-6323-6 |
JIS G 3445 | DIN 17177 EN 10217-1 AND 2 EN 10305-2 AND 3 |
ASTM A423 GR.1 ASTM A214 |
Products application
They are utilized in very corrosive environments.
• Extremely Corrosive Corten B pipes and tubes are employed in a variety of processing-related enterprises and sectors,
including sugar mills, fertilizer factories, chemical plants, and power plants.
• Most commonly, air pre heaters, steam generating boilers,heat exchanger and economiser employ Corten B pipes and tubes.