Q500NH Weather Resistant Steel Plate

Q500NH Weather Resistant Steel Plate

Q500NH Weather Resistant Steel Plates, also known as low alloy steels, are steels with a carbon content of less than 0.2% by weight. To which Cu, Cr, Ni.P, Si and Mn are mainly added as alloying elements, totaling no more than 3-5% wt. The chemical composition of these steel alloys is specially formulated to provide early formation of rust/iron oxide layer to provide weatherproof coating to the underlying steel.
Send Inquiry
Description
Technical Parameters

Products Description

 

 

Designation Method for Q500NH Weather Resistant Steel Plate:

 

The designation for Q500NH steel plate consists of:

- "Q" (first letter of "Yield strength" in Chinese pinyin)

- "NH" (first letters of 'corten" in Chinese pinyin)

- Minimum yield strength value

- Quality grade (A, B, C, D, E)

 

Example: Q500NH

Q -- Yield strength

500 - Lower yield strength limit of steel, in MPa;

NH - Abbreviation for weather-resistant steel in Chinese;

A, B, C, D, E - Quality grades.

Q500NH Steel Plate

2. Q500NH Weathering steel plate compliance standard: GB/T 4171-2008.

 

Q500NH Steel Plate

 

3. Delivery condition of Q500NH high strength corten steel plate: Supplied in hot-rolled, controlled-rolled, or normalized condition; may also be supplied in quenched and tempered condition.

 

Chemical Composition of GB/T 4171 Q500NH Weathering Steel Plate

 

 

C

Si

Mn

P

S

Cu

Cr

Ni

0.12

0.65

2

0.025

0.03

0.25-0.55

0.30-1.25

0.12-0.65

 

GB/T 4171 Q500NH Weathering Steel Plate Mechanical Properties

 

 

Tensile Strength(MPa)

Yield Strength(MPa)

Elongation %

600-760

500

18

 

Technical Requirements & Additional Services

 


♦ High tension test


♦ Low temperature impacting test


♦ Simulated post-welded heat treatment (PWHT)


♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2


♦ Shot blasting and Painting, Cutting and welding as per end user's demands


♦ G101 Guide for estimating atmospheric corrosion resistance of low alloy steels

 

Other Terms

 

 

Packaging Details: Standard export seaworthy packing or as required.


Delivery Time: 30-50 days, 7 days for stock goods.


Loading Port: Shanghai ,Tianjin, Qingdao.


Offer Ability:5 000MT/Per Month.


MOQ: 1 Pcs.

Packing Corten

Contact now to get Q500NH Quote

 

About Us

 

 

 

Transitioning from a pure trading exporter to an integrated manufacturing service provider, Gnee has undergone multiple strategic transformations.

 

Between 2010 and 2013, the company focused on enhancing fabrication capabilities by investing in laser cutting and bending equipment, launching precision processing.

 

Starting in 2016, Gnee took on large-scale custom engineering projects, boosting project management and R&D.

 

By 2019, Gnee's clients spanned over 100 countries, significantly increasing brand influence internationally.

 

With overseas offices established in 2021, the company's global footprint improved further.

 

Looking ahead, Gnee continues to emphasize green sustainability and technological innovation to drive industry advancement.

 

 

Gnee Corten

Hot Tags: q500nh weather resistant steel plate, China q500nh weather resistant steel plate manufacturers, suppliers, corten plate, A242 Corten Steel, A709 Weathering Plate, High Tensile Weathering Steel, A588 steel sheet, cutting corten steel