S235J0W Atmospheric Corrosion Resistance Steel Plate

S235J0W Atmospheric Corrosion Resistance Steel Plate

S235J0W Atmospheric Corrosion Resistance Steel Plate has the material designation 1.8958, conforms to the EN 10025-5 standard, and belongs to the category of structural steels with improved atmospheric corrosion resistance. It is commonly referred to as weathering steel or atmospheric corrosion-resistant steel.
Send Inquiry
Description
Technical Parameters

Products Description

 

S235J0W Atmospheric Corrosion Resistance Steel PlateS235J0W Atmospheric Corrosion Resistance Steel Plate has the material designation 1.8958, conforms to the EN 10025-5 standard, and belongs to the category of structural steels with improved atmospheric corrosion resistance.

 

It is commonly referred to as weathering steel or atmospheric corrosion-resistant steel.

 

A key characteristic of this steel is that when exposed to the atmosphere, its surface gradually forms a dense, stable protective oxide layer (rust layer).

 

This layer significantly slows subsequent corrosion, making its corrosion resistance far superior to ordinary carbon steel.

 

Regarding mechanical properties, S235J0W exhibits a minimum yield strength of 235 MPa (applicable to plates ≤16 mm thick), with tensile strength typically ranging from 360–510 MPa and elongation not less than 26%.

 

These metrics ensure a favorable balance between load-bearing capacity and ductility, making it suitable for diverse welding and structural fabrication applications.

S235J0W High Strength Atmospheric Corrosion Resistance Steel Plate

For impact performance, the "J0" designation indicates a Charpy V-notch impact absorption energy of no less than 27 J at 0°C, ensuring sufficient toughness and safety in low-temperature environments.

 

Regarding atmospheric corrosion resistance, S235J0W Corten Steel Plate exhibits a corrosion rate significantly lower than ordinary carbon steel. Under industrial atmospheric or marine climates, its average annual corrosion depth typically ranges from 0.01–0.03 mm/year, whereas ordinary carbon steel often exceeds 0.1 mm/year.

 

This property enables S235J0W Weatherig Steel Plate to significantly reduce maintenance frequency during long-term outdoor exposure, extending its service life by 3–5 times compared to conventional carbon steel.

 

Consequently, S235J0W Hot Rolled Corten Steel Plate is extensively used in bridges, building curtain walls, railway vehicles, containers, towers, and various welded structures. It is particularly suitable for engineering applications in rainy, windy, and saline environments.

 

Specification

 

Gangsteel Grade :

S235J0W Hot Rolled Weathering Steel Plate

Specification:

Thickness 8mm-300mm, Width: 1500-4020mm, Length: 3000-27000mm

Standard:

EN10025-5 Technical delivery conditions for general structural steels

Approval By Third Party

ABS, DNV, GL, CCS, LR , RINA, KR, TUV, CE

Classification:

hot rolled or normalizing structural steels

 

Chemical composition % of the Product analysis of grade S235J0W

 

C

Si

Mn

Cu

P

S

Cr

N

0.16

0.45

0.15-0.70

0.20-0.60

0.040

0.040

0.35-0.85

0.010

 

Mechanical properties of grade S235J0W

 

Temperature

-20

-10

0

20

Notch impact test. Min. absorbed energy J

 

 

27

 

 

Nominal thickness (mm)

to 16

16 - 40

40 - 63

63 - 80

80 - 100

100 - 150

ReH - Minimum yield strength (MPa)

235

225

215

215

215

195

 

Nominal thickness (mm)

to 3

 

3 - 100

 

100-150

Rm -Tensile strength (MPa)

360-510

 

360-510

350-500

 

Nominal thickness (mm)

≥1.5<2

≥2﹤2.5

 

≥2.5<3

 

≥3<40

≥40﹤63

≥6﹤100

≥100﹤150

A - Minimum elongation Lo = 5,65 √ So (%) Longitudinal

 

19

 

20

 

21

 

26

 

25

 

24

 

22

 

Equivalent grades of grade S235J0W

 

UNI

EU 155

France

NFA35502

Germany

WBL 087

U.K.

BS 4360

Canada

CSA G4021

USA

ASTM

Fe360 CK1

E 24W3

WSt 37-2

 

 

 

 

 

S235J0W steel main application

 

s235j0w bridges

S235J0W High Strength Atmospheric Corrosion Resistance Steel Plate is used for shipping containers,steel bridges,vessels and tanks for preventing atmospheric corrosion usage.

 

Contact now to get S235J0W Quote

 

Hot Tags: s235j0w atmospheric corrosion resistance steel plate, China s235j0w atmospheric corrosion resistance steel plate manufacturers, suppliers, Laser Cut Corten Steel Sheet, Acid Resistant Steel Plate, cutting corten steel, Sea Water Corrosion Resistant Corten Plate, Cold Rolled Corten Sheet, Corten Steel Laser Cutting