Product Description

Corten A is a high-strength, low-alloy weathering steel specifically developed for structural applications that require enhanced resistance to atmospheric corrosion.
When exposed to open air, Corten A Plate naturally develops a protective rust-colored surface layer (patina), which acts as a shield against further oxidation, eliminating the need for painting or surface coatings.
As a trusted and experienced supplier, we offer Corten A Weathering Steel Plate in a wide range of thicknesses, widths, and lengths.
Our products meet international quality standards and are suitable for heavy-duty, structural, and aesthetic applications.
Features

✅ Atmospheric Corrosion Resistance
Forms a self-protective oxide layer when exposed to the environment
Ideal for outdoor and exposed applications with minimal maintenance
✅ High Strength & Structural Reliability
Superior yield and tensile strength for load-bearing performance
Suitable for demanding structural designs
✅ Distinctive Aesthetic
Natural rust-like finish develops over time
Popular in modern architecture and design
✅ Excellent Workability
Can be welded, cut, bent, and formed
Compatible with standard fabrication processes
Available Dimensions
|
Parameter |
Range |
|
Thickness |
1 mm – 300 mm |
|
Width |
Up to 2500 mm |
|
Length |
Up to 18000 mm |
|
Surface |
Rusted / Mill Finish / Cleaned |
|
Form |
Plates / Sheets / Cut-to-size |
Mechanical Properties
|
Property |
Value |
|
Yield Strength |
345–355 MPa (depending on thickness) |
|
Tensile Strength |
470–630 MPa |
|
Elongation |
≥ 20% |
|
Hardness |
Typically 165–185 HBW |
|
Thickness Range |
1 mm – 300 mm |
Chemical Composition (Corten A)
|
Element |
Composition (%) |
|
Carbon (C) |
≤ 0.16 |
|
Silicon (Si) |
0.30 – 0.50 |
|
Manganese (Mn) |
0.80 – 1.25 |
|
Phosphorus (P) |
≤ 0.030 |
|
Sulfur (S) |
≤ 0.030 |
|
Chromium (Cr) |
0.40 – 0.65 |
|
Copper (Cu) |
0.25 – 0.40 |
|
Vanadium (V) |
0.02 – 0.10 |
|
Nickel (Ni) |
≤ 0.40 |
Technical Conditions

Ultrasonic Tested: As per SA 578 or as required
Material Test Certificate (MTC): As per EN 10204 / 3.2
Impact Testing: Charpy tested at –20°C / –46°C
Heat Treatment: Furnace Normalized
Documentation: Gnee plates available with IBR Form IV
Applications of Corten A Plate

Building facades & cladding systems
Structural frameworks & bridges
Industrial chimneys & containers
Outdoor art, sculptures, and signage
Marine and harbor structures
Architectural landscaping elements
Corten A's natural aging process and low maintenance needs make it a preferred material in modern architecture, civil infrastructure, and industrial design.
Why Choose Our Corten A Weathering Steel Plate?
- Only supplies authentic Corten A - no substitutes
- In-stock availability and fast worldwide delivery
- Support for CNC cutting, pre-rusting, edge prepping
- Full technical certification & traceability
- Backed by years of expertise in Corten A supply & processing
We are your reliable partner for High Strength Corten A Weathering Steel Plate in both structural and aesthetic applications.
Hot Tags: high strength corten a weathering steel plate, China high strength corten a weathering steel plate manufacturers, suppliers, laser cut corten, Corten A Steel Coil, 09CrCuSb Corten Plate, Acid Resistant Steel Plate, ASTM Weathering Steel Plate, Corten A coil