S355J2WP Corten Steel Sheet

S355J2WP Corten Steel Sheet

S355J2WP Corten Steel is a hot-rolled structural steel developed for applications requiring high resistance to atmospheric corrosion. Alloyed with chromium, copper, and phosphorus, it forms a stable patina layer on the surface when exposed to weather.
Send Inquiry
Description
Technical Parameters

S355J2WP Corten Steel is a hot-rolled structural steel developed for applications requiring high resistance to atmospheric corrosion. Alloyed with chromium, copper, and phosphorus, it forms a stable patina layer on the surface when exposed to weather.

 

product-455-459

 

This rust-like coating prevents further corrosion, effectively extending the steel's service life without the need for painting or maintenance.

 

Engineered for structural durability and environmental resilience, S355J2WP Corten Steel Plate is widely used in bridges, infrastructure, architectural facades, and welded heavy-duty applications.

 

Specifications

 

 

product-605-461

 

Thickness: 6mm – 250mm

 

Width: 1650mm – 3700mm

 

Length: 3000mm – 18000mm

 

Delivery Conditions: +N (Normalized) / +AR (As Rolled)

 

Tests: HIC, Z15/Z25/Z35, UT, -20°C Charpy V-Notch

 

 

Chemical Composition (% by weight)

 

 

Element

C ≤

Si ≤

Mn ≤

P

S ≤

Cr

Cu

Content

0.12

0.75

1.00

0.06–0.15

0.030

0.30–1.25

0.25–0.55

*May contain micro-alloying elements such as Nb, V, Ti, or Al to enhance performance.

 

Mechanical Properties

 

 

Property

Value

Yield Strength

≥355 MPa (for t ≤ 16 mm)

Tensile Strength

510–680 MPa

Elongation

≥19% (varies by thickness)

Impact Toughness

27J at -20°C

 

Features

 

 

product-603-456

✅ Self-Protecting Rust Layer
Forms a dense oxide film that shields the steel surface from further degradation, eliminating the need for protective coatings.

 

✅ Excellent Structural Strength
With a yield strength of ≥355 MPa and tensile strength ranging from 510 to 680 MPa, S355J2WP Weathering Steel Plate is suitable for demanding load-bearing applications.

 

✅ Reliable in Harsh Environments
Performs well in coastal, industrial, and high-humidity environments where conventional carbon steel may corrode rapidly.

 

product-453-455

 

 

✅ Superior Weldability and Workability
Easy to cut, weld, and form using standard processes, making it ideal for both factory fabrication and on-site construction.

 

✅ Architectural Appeal
Its naturally weathered appearance provides an attractive, earthy aesthetic often used in exposed structures and modern design.

 

 

 

 

Applications

 

 

product-606-457

S355J2WP Corten Steel Plate is intended for use in welded structures subjected to outdoor exposure and dynamic loading, such as:

 

Bridge beams, decks, and safety railings

 

Hydraulic structures (e.g., floodgates, spillways)

 

Storage tanks, water towers, and silos

 

Architectural panels and cladding systems

 

Industrial chimneys, pylons, containers, and rail wagons

 

 

We offer customized cutting and processing services for S355J2WP Weathering Steel Plate and maintain large inventories for fast delivery.

product-453-456

Material test certificates (MTC) and inspection reports are available upon request. Contact us today for pricing, technical support, or to request samples.

Contact now

 

Hot Tags: s355j2wp corten steel sheet, China s355j2wp corten steel sheet manufacturers, suppliers, corten steel sheet metal, High Strength Weathering Steel Plate, Sea Water Corrosion Resistant Corten Plate, High Tensile Weathering Steel, Sulfuric Acid Resistant Corten, Corten metal sheet