09CrCuSb (ND steel) is a low-alloy corrosion-resistant steel developed for manufacturing seamless steel tubes used in sulfur-containing corrosive environments.
By adding alloying elements such as chromium, copper, and antimony to carbon steel, ND steel significantly improves resistance to sulfur corrosion and high-temperature flue gas attack, effectively extending the service life of equipment.

This material is widely used in power plants and oil refineries, especially in equipment that operates for long periods under high temperature and corrosive gas conditions.
Typical applications include economizers, air preheaters, heat exchangers, and evaporators, where strong resistance to sulfur-rich flue gas is essential for stable operation.
Mechanical Properties of ND Steel (09CrCuSb)
| Property | Value |
|---|---|
| Tensile Strength | 390–550 MPa |
| Yield Strength | ≥ 245 MPa |
| Elongation | ≥ 25% |
Chemical Composition of ND Steel (09CrCuSb)
| Element | Content (%) |
|---|---|
| Carbon (C) | ≤ 0.10 |
| Silicon (Si) | 0.20 – 0.40 |
| Manganese (Mn) | 0.35 – 0.65 |
| Chromium (Cr) | 0.70 – 1.20 |
| Copper (Cu) | 0.25 – 0.45 |
| Antimony (Sb) | ≤ 0.10 |
| Sulfur (S) | ≤ 0.10 |
| Phosphorus (P) | ≤ 0.10 |
09CrCuSb (ND steel) is often regarded as an equivalent to weathering steel or Corten steel in terms of corrosion resistance. In sulfur corrosion environments, its performance is particularly outstanding compared with ordinary carbon steel, making it a reliable alternative for demanding industrial conditions.
As a weathering-type low-alloy steel, ND steel forms a dense and stable protective oxide layer on its surface when exposed to the atmosphere. This natural protective layer slows down further corrosion and prevents rapid metal loss, ensuring long-term structural integrity and improved safety.
In addition to its excellent corrosion resistance, 09CrCuSb steel offers good mechanical strength and ductility. This balance of properties allows the material to withstand mechanical loads while maintaining good formability and weldability, making it well suited for seamless tube production and industrial fabrication.
From an economic perspective, ND steel does not require additional painting or anti-corrosion coatings. Its self-protective surface significantly reduces maintenance and repair costs over the entire service life, offering clear cost advantages compared with conventional carbon steel.
Environmentally, 09CrCuSb (ND steel) supports sustainable development goals. By minimizing the need for chemical coatings and frequent maintenance, it reduces environmental impact while improving the long-term efficiency of industrial systems.
Overall, 09CrCuSb (ND steel) is a high-performance corrosion-resistant material designed for high-temperature and sulfur-containing environments. It is an ideal choice for power generation and petrochemical applications, providing durability, reliability, and economic efficiency beyond that of ordinary carbon steel.

What is 09CrCuSb steel?
09CrCuSb, also known as ND steel, is a low-alloy corrosion-resistant steel specially designed for use in acidic dew point corrosion environments. It contains alloying elements such as chromium (Cr), copper (Cu), and antimony (Sb), which significantly enhance its resistance to sulfuric acid and flue gas corrosion.
Why is 09CrCuSb called ND steel?
"ND" stands for Nitric acid and Dew-point corrosion resistance. The steel was developed to withstand low-temperature acid condensation corrosion commonly found in boilers, heat exchangers, and flue gas systems.
Does 09CrCuSb steel have good weldability?
Yes. 09CrCuSb steel has good weldability. Standard welding methods such as SMAW, SAW, and TIG can be used, but low-hydrogen electrodes and proper preheating may be recommended for thicker sections.
Is 09CrCuSb suitable for high-temperature service?
09CrCuSb is mainly designed for medium-temperature environments where acid dew point corrosion occurs. It is not intended for extremely high-temperature pressure vessel applications without proper evaluation.