Products Description
ASTM A709-50W is a standard specification for structural steel primarily in the fabrication of steel bridges. ASTM A709-50W covers high strength, low allow steel structural shapes, plates and bars.
The atmospheric corrosion resistance of this steel in most environments is substantially better than carbon steel with or without copper addition. ASTM A709-50W shall have an atmospheric corrosion index of 6.00 or higher.
The chemistry of an astm a709 gr 36 steel Seamless Pipe may contain any of the following elements carbon, sulfur, silicon, manganese, phosphorus, and copper in a specified limit.

A tension test administered on the astm a709 grade 50 steel pipe could be used to circumscribe the expected tensile properties. Generally, tensile tests detail parameters such as tensile and yield strength in addition to elongation properties as well. Materials for the astm a709 grade 50w weathering steel Pipe are mandated to undergo the following tests.
First, an impact test is conducted on the specimen for both the non-fracture critical as well as the fracture critical members. Next, the specimen of ASTM A709 Pipe is subjected to a Brinell hardness test for Grades 100 and 100W. It is required to check the ASTM A709 Grade 50W Pipe for atmospheric corrosion resistance.
Products Specification
|
Production |
ASTM A709 Steel pipe |
|
Standard |
ASTM |
|
Out Diameter |
DN10~DN1200,1/8"~100",6mm~2400mm |
|
Wall Thickness |
SCH5~SCH160,STD,XS,XXS,1mm~120mm |
|
Material |
ASTM A106 GRB/ A53 GRB/ API 5L X42,X52,X60,X65,X70GRB/ API 5 CT/ Q345/ ST42/ST37/ ST52.Q195/Q215/Q235/A179etc. |
|
Length |
12m,11.8m,6m,5.8m,or as customers required |
|
Surface treatment |
Black painting, black varnish, transparent oil, hot galvanized, 3PE,epoxy coating,BE,PE.etc. |
|
Technique |
Seamless & welded |
|
Usage |
1. Low and middle pressure fluid transportation pipeline 2. Casing Tube 3. Boiler Pipe 4. Petroleunm and natural gas industry 5. Chemistry industry 6. Electric industry |
|
Package |
1. Bundle packing. 2. Bevelled end or plain end or warnished as per buyer's required. 3. Marking: as per customer's requests. 4. Painting varnish coating on the pipe. 5. Plastic caps at ends. |
|
Supply |
1. seamless steel pipe 2. ERW steel pipe 3. steel casing 4. tubing 5. hot-rolled steel pipe 6. spiral steel pipe 7. hot-galvanized steel pipe |
|
Min Order Quantity |
According to customer's requirement |
impact properties of ASTM A709 gr 36 steel Seamless Pipe
| GRADE | THICKNESS (in) |
MIN LONGITUDINAL INDIVIDUAL VALUE 1) (ft-lbs) |
MIN LONGITUDINAL AVERAGE ENERGY 1) (ft-lbs) |
ZONE 2 TEST TEMP | ZONE 1 TEST TEMP | ZONE 3 TEST TEMP |
|---|---|---|---|---|---|---|
| HPS 50WT | 0.50 – 2.00 | - | 20 | 10 oF | 10 oF | 10 oF |
| HPS 50WF | 0.50 – 2.00 | 24 | 30 |
mechanical properties
| GRADE | THICKNESS (in) |
ELONGATION IN 8″ 2) (MIN %) |
TENSILE STRENGTH (MIN ksi) |
YIELD STRENGTH 1) (MIN ksi) |
ELONGATION IN 2″ 2) (MIN %) |
|---|---|---|---|---|---|
| HPS 50W | 0.50 – 2.00 | 18 | 70 | 50 | 21 |
Chemical properties of ASTM A709 grade HPS 50W
| TYPE | MN (wt %) |
C (MAX wt %) |
S (MAX wt %) |
P (MAX wt %) |
MO (wt %) |
ALTOT (wt %) |
SI (wt %) |
V (wt %) |
CU (wt %) |
CR (wt %) |
N (MAX wt %) |
NI (wt %) |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| HPS 50W | 0.10 – 1.35 | 0.11 | 0.006 | 0.020 | 0.02 – 0.08 | 0.010 – 0.040 | 0.30 – 0.50 | 0.04 – 0.08 | 0.25 – 0.40 | 0.45 – 0.70 | 0.015 | 0.25 – 0.40 |
Available sizes Of ASTM A709 Pipe
| GRADE | THICKNESS | WIDTH | LENGTH |
| 36 | 3/16" – 4" | 48" – 120" | UP TO 480" |
| 50 | 3/16" – 4" | 48" – 120" | UP TO 480" |
| 50W | 3/16" – 4" | 48" – 120" | UP TO 480" |