How about the Q295GNH Corten Steel Plate

Sep 15, 2025 Leave a message

Products Description

 

Q295NH weathering steel plateQ295GNH Corten Steel Plate is an atmospheric corrosion-resistant steel, also known as corten steel. It is made from ordinary carbon steel with the addition of approximately 0.25% copper, 0.30% nickel, and other corrosion-resistant elements.

 

Q295NH weathering steel plate has the characteristics of high-quality steel, including a yield strength ≥ 295 MPa, tensile strength of 440–580 MPa, toughness (room temperature impact energy ≥ 27 J), as well as excellent ductility, formability, weldability, and machinability, along with wear resistance, high-temperature resistance, and fatigue resistance.

 

Meanwhile, Q295NH weathering steel also offers corrosion protection, extended service life (typically over 30 years), material thinning, and reduced consumption.

 

GBT4171 Q295NH corten steel plate chemical composition

 

C Si Mn P S Cu Ni Cr
0.15 0.10-0.50 0.30-1.00 0.03 0.03 0.25-0.55 0.65 0.40-0.80

 

GBT4171 Q295NH weathering steel sheet mechanical property

 

Q295NH ≤ 16 > 16 ≤ 40 > 40 ≤ 60 >60
Yield strength (≥Mpa) 295 285 275 255
Tensile strength (Mpa) 430-560
Elongation 24 24 23

 

22

 

Application

Q295NH weathering steel plate is primarily used in railways, vehicles, bridges, towers, and other steel structures that are exposed to atmospheric conditions for extended periods.

 

The plate thickness typically ranges from 6 to 50 mm, with a yield strength of over 295 MPa, tensile strength between 440 and 580 MPa, and room temperature impact energy ≥ 27 J.

 

It combines excellent toughness, ductility, and fatigue resistance, making it suitable for projects requiring high load-bearing capacity, impact resistance, and long-term durability.

 

Q295NH weathering steel plate is also widely used in the manufacture of containers, railway vehicles, oil platforms, port buildings, and containers for chemical and petroleum equipment exposed to corrosive media such as sulfur and argon.

 

In these applications, Q295NH weathering steel can significantly extend service life (typically over 30 years), reduce material consumption and maintenance costs, while maintaining strong structural safety and durability.

Q295NH Weathering Steel

Our Q295NH weathering steel plate advantage

 

1. Best Quality-Our steel from China First-Class mill with Die stamp include heat number and batch number,It can be tracked.


2. Fast Delivery-Good relationship with Mill and Forwarder Shipping Agent for producing and shipping.


3. Professional Team-Work steel business more than six years for export steel plate.


4. Reasonable Price-Cooperate with 15 mills, satisfy with different request for the price and quality.


5. Kinds of Payment-T/T, L/C at sight, Usance Letter of Credit.

 

If you want to know more information about Q295NH weathering steel plate, please contact us and let us know your required Q295NH weathering steel specification, the best Q295NH weathering steel plate price will be quoted in shortest time.

 

Contact now to get Q295NH Quote