1. Rough, Scale-Covered As-Rolled Surface: Impacts on Aesthetic and Architectural Applications
The natural hot-rolled surface features a coarse texture with a thick iron oxide mill scale and uneven coloration, along with minor surface defects like roll marks and pits. This finish limits direct use in high-end architectural decorative applications (e.g., building facades, exterior trim) that require uniform visual effects, as it causes uneven patina formation in the early outdoor exposure stage-localized rusting and discoloration occur due to scale peeling, leading to inconsistent aesthetic results. It is only suitable for non-visible architectural structural components where appearance is not a priority.

2. Rough, Scale-Covered As-Rolled Surface: Advantages for Industrial/Structural Applications
For industrial and heavy structural applications, the rough hot-rolled surface and mill scale bring practical benefits. The coarse texture improves the adhesion of concrete, mortar and protective coatings (e.g., paint, anti-corrosion primer) if surface treatment is required, preventing coating peeling or concrete debonding under dynamic loads or environmental impacts. Additionally, the mill scale provides a temporary initial protection for steel plates during short-term storage and transportation, reducing early rusting before on-site processing and installation.

3. Pickled & Descaled Hot-Rolled Surface: Expanded Architectural and General Fabrication Use
After pickling, the hot-rolled SPA-H surface has mill scale and oxide layers removed, presenting a relatively clean, matte metallic finish (still rougher than cold-rolled plates, with no high smoothness). This treated finish eliminates the uneven patina issue of the as-rolled surface, enabling uniform natural rust formation in outdoor environments-it can be used for mid-range architectural applications (e.g., landscape structures, industrial park building cladding) that pursue natural weathering aesthetics but do not require ultra-smooth surfaces. It also simplifies subsequent processing (e.g., welding, punching) by removing scale that would cause weld spatter or tool wear.

4. Hot-Rolled Surface Roughness: Impacts on Processing and Secondary Fabrication
The inherent surface roughness of hot-rolled SPA-H (whether as-rolled or pickled) affects secondary fabrication processes differently than cold-rolled plates. On one hand, the rough surface increases friction during forming processes (e.g., bending, rolling), requiring higher processing force and increasing wear on molds and cutting tools, which needs more frequent tool maintenance for mass production. On the other hand, the roughness avoids surface slippage during mechanical fixing (e.g., bolted connection, riveting), improving the stability of fastener joints and reducing the risk of loosening under vibration (e.g., in bridge railings, industrial equipment frames).

5. Surface Defect Sensitivity: Impacts on Corrosion Resistance in Specific Environments
Minor surface defects (e.g., pits, roll marks, scale gaps) on hot-rolled SPA-H are unavoidable in the as-rolled state. In mild atmospheric environments, these defects do not affect the long-term formation of a dense protective patina-the patina will eventually cover and repair small defects. However, in harsh corrosive environments (e.g., high-humidity coastal areas with salt spray, industrial zones with acid mist), these defects become initial micro-corrosion points, accelerating localized oxidation and pitting corrosion before the patina is fully formed. For such applications, the hot-rolled surface must undergo additional treatment (e.g., pickling, anti-corrosion priming) to eliminate defects and ensure consistent corrosion resistance.








