Cold Rolled Corten Steel Coil

Cold Rolled Corten Steel Coil

Cold Rolled Corten Steel Coil is a premium product manufactured from high-strength low-alloy weathering steel through cold rolling processing. The cold rolling process delivers superior dimensional accuracy, enhanced surface finish, and improved mechanical properties.
Send Inquiry
Description
Technical Parameters

Product Description

 

Cold Rolled Corten Steel Coil is a premium product manufactured from high-strength low-alloy weathering steel through cold rolling processing. The cold rolling process delivers superior dimensional accuracy, enhanced surface finish, and improved mechanical properties. Its unique alloy composition provides excellent atmospheric corrosion resistance, allowing the coil to naturally develop a stable and dense rust patina in harsh environments, preventing further corrosion without the need for additional coatings.

This cold rolled weathering steel coil is not only structurally robust but also features a smooth surface, making it ideal for applications requiring high precision and aesthetic appeal. It is widely used in architectural cladding, bridge structures, landscaping, transportation facilities, industrial equipment, and more, fulfilling various engineering and decorative needs.

Gnee is dedicated to supplying high-quality cold rolled Corten steel coils, offering customization in thickness and width to ensure every coil meets international standards and client specifications.

 

Product Detail

 

image001
image003
image005
image007
image009
image011

 

Corten steel cold rolled coils chemical properties

 

 

Si % max.

C % max.

Mn %

Z %

S % max.

P %

N % max.

Cr %

V %

Cu %

Ni %

Mo %

According to EN 10027-1

S235J2W

0.40

0.13

0.20-0.60

–

0.03

0.04

–

0.40-0.80

–

0.25-0.55

0.65

–

S235J0W

0.40

0.13

0.20-0.60

–

0.04

0.04

0.01

0.40-0.80

–

0.25-0.55

0.65

–

S355J2WP

0.75

0.12

1.00

–

0.03

0.06-0.15

–

0.30-1.25

–

0.25-0.55

0.65

–

S355J0W

0.75

0.12

1.00

–

0.04

0.06-0.15

0.01

0.30-1.25

–

0.25-0.55

0.65

–

S355J2W

0.50

0.16

0.50-1.50

0.15

0.03

0.03

–

0.40-0.80

–

0.25-0.55

0.65

0.30

S355J0W

0.50

0.16

0.50-1.50

0.15

0.04

0.04

0.01

0.40-0.80

–

0.25-0.55

0.65

0.30

S355K2W

0.50

0.16

0.50-1.50

0.15

0.03

0.03

–

0.40-0.80

–

0.25-0.55

0.65

0.30

According to ASTM & ASME Specn.

A 588 Gr. B

0.15-
0.50

0.20

0.75-1.35

 

0.05

0.04

–

0.40-0.70

0.01-
0.10

0.20-0.40

   

A 588 Gr. A

0.3-
0.65

0.19

0.80-1.25

 

0.05

0.04

–

0.40-0.65

0.02-
0.10

0.25-0.40

   

 

What is corten steel coil used for?

 

Corten steel can be used for various outdoor structural and architectural applications due to its unique properties and appearance:

  • Corten steel coil has good aesthetic appeal and can be used in architectural elements like facades, cladding, etc.
  • They can be used in bridge construction for their high strength and corrosion resistance.
  • Due to its weathered appearance, it can be used in outdoor sculptures and artworks.
  • Landscaping features like retaining walls, planters, etc. due to its durability and rustic appearance.
  • Shipping containers and other transportation applications for their weather resistance and strength.

 

Hot Tags: cold rolled corten steel coil, China cold rolled corten steel coil manufacturers, suppliers, ACR Corten Steel Plate, Hot rolled Corten A coil, Cold Rolled Corten Sheet, Hot Rolled Corten Plate, corrosion resistant steel, Corten steel perforated panels