S355J0WP steel and S355J2WP Weather Resistant Steel Plate fall under the European standard EN10025-5 for atmospheric corrosion-resistant steel, forming a protective rust layer on their surfaces to resist atmospheric corrosion.
By adding specific alloying elements (such as P, Cu, Cr, Ni, Mo) to the steel, a self-generating protective oxide layer forms on the base metal surface under climatic conditions, thereby enhancing resistance to atmospheric corrosion.
In urban environments, both grades exhibit corrosion rates of approximately 0.02 mm/year, rising to 0.03–0.04 mm/year in coastal or salt spray conditions-significantly lower than the 0.1–0.15 mm/year typical for ordinary carbon steel.
Their naturally formed rust layers typically achieve full stability within 12–24 months, extending steel service life to 40–60 years and significantly reducing coating and maintenance costs.
S355J0WP and S355J2WP steel plates are suitable for manufacturing low-alloy structural steel components such as vehicles, bridges, towers, containers, and storage tanks.
S355J2WP steel sheet exhibits tensile strength of 510–680 MPa, yield strength ≥355 MPa, and elongation ≥20%, while S355J0WP high strength corten steel plate offers tensile strength of 470–630 MPa, yield strength ≥355 MPa, and elongation ≥22%.
This enables both grades to not only deliver outstanding corrosion resistance but also meet the load-bearing requirements for bridges, railways, and other outdoor structures.
Chemical composition of S355J0WP steel and S355J2WP plate (melting analysis)
Grades |
C |
Si |
Mn |
P |
S |
N |
Cr |
Cu |
|
S355J0WP |
≤0.15 |
≤0.80 |
≤1.1 |
0.05-0.16 |
≤0.040 |
≤0.010 |
0.25-1.35 |
0.20-0.60 |
|
S355J2WP |
≤0.15 |
≤0.80 |
≤1.1 |
0.05-0.16 |
≤0.035 |
- |
0.25-1.35 |
0.20-0.60 |
Mechanical properties comparison
Grades |
Yield strength ReHa, MPab |
Tensile strength Rma, MPab |
|||||||
|
Thickness, mm |
Thickness, mm |
||||||||
|
EN 10027-1;CR 10260 |
£ 16 |
16-40 |
40-63 |
63-80 |
80-100 |
100-150 |
£3 |
3-100 |
100-150 |
|
S355J0WP |
355 |
345 |
- |
- |
- |
- |
510-680 |
470-630 |
- |
|
S355J2WP |
|||||||||
Longitudinal impact strength
Grades |
Temperature℃ |
Energy,J |
|
S355J0WP |
0 |
27 |
|
S355J2WP |
-20 |
27 |