SPA-H weathering steel (JIS G3125) is a low-alloy atmospheric corrosion-resistant steel. Its core corrosion resistance comes from a carefully balanced set of alloying elements, with Cu, Cr, Ni, and P being the most critical for forming a stable protective patina. Below are the main elements, their typical ranges, and key functions:
 

1. Core Weathering Elements (Key for Patina & Corrosion Resistance)

 
Element Typical Range Primary Function
Copper (Cu) 0.25–0.55% The primary corrosion-resistant element; enriches in the patina, forms a dense oxide barrier, and blocks moisture/oxygen penetration.
Chromium (Cr) 0.40–0.65% Enhances passivation, stabilizes the patina, and improves resistance to mild acids and pollutants.
Nickel (Ni) ≤0.65% Boosts overall corrosion resistance, improves toughness, and prevents "copper brittleness" in hot working.
Phosphorus (P) ≤0.035% Promotes uniform, dense patina formation; synergizes strongly with Cu/Cr to slow rust propagation.

info-330-302

 

 

2. Basic Structural & Process Elements

 
Element Typical Range Primary Function
Carbon (C) ≤0.16% Controls strength and hardness; kept low to preserve weldability and toughness.
Silicon (Si) ≤0.55% Aids early oxide layer formation and strengthens the steel matrix.
Manganese (Mn) ≤1.40% Improves strength, toughness, and hot workability; deoxidizes the melt.
Sulfur (S) ≤0.035% Strictly limited as an impurity to avoid brittleness and surface defects.