If you're selecting materials for a structural project, understanding the fundamental strength of S355W Corten steel is key. This grade balances weather resistance with reliable load-bearing capacity.
The Core Strength Specifications
For S355W weathering steel, the minimum yield strength and tensile strength are defined by the European standard EN 10025-5. A critical detail is that the minimum yield strength varies depending on the thickness of the steel plate.
The following table outlines how the yield strength (ReH) changes with thickness, alongside the consistent tensile strength (Rm) range:
| Nominal Thickness (mm) | Minimum Yield Strength (ReH) | Tensile Strength (Rm) Range |
|---|---|---|
| Up to 16 | 355 MPa | |
| >16 to 40 | 345 MPa | 470 - 630 MPa |
| >40 to 63 | 335 MPa | |
| >63 to 80 | 325 MPa | |
| >80 to 100 | 315 MPa |

Why This Matters for Your Design:
Yield Strength (ReH) is the stress at which the steel begins to deform permanently. You use this value to ensure your structure maintains its shape under load. The "355" in S355W denotes a minimum yield strength of 355 MPa for sections up to 16mm thick.
Tensile Strength (Rm) is the maximum stress the steel can withstand while being stretched. The range of 470-630 MPa indicates its overall strength and ductility.
Understanding the "S355W" Name
The naming convention is a direct code to its properties:
S: Stands for "Structural" steel.
355: Indicates the minimum yield strength in MPa (for thickness ≤16mm).
W: Signifies "Weathering" resistance, meaning it forms a protective rust patina.
Comparing Common S355 Weathering Grades
S355W is part of a family. The suffix letters and numbers (like J0, J2, K2) indicate differing toughness levels for impact resistance, which is crucial for low-temperature applications.
| Grade | Key Difference from S355W | Typical Application Context |
|---|---|---|
| S355J0W | Guaranteed impact resistance at 0°C. A common, general-purpose weathering steel. | General construction, facades, and structures in moderate climates. |
| S355J2W | Guaranteed impact resistance at -20°C. Offers better low-temperature toughness. | Bridges, exposed structures, or applications in colder regions. |
| S355K2W | Similar to S355J2W but with different manufacturing controls for guaranteed toughness. | Heavy-duty structures where superior impact properties are specified. |
Selecting the Right Grade for Your Project
Choosing between these grades depends on your project's environment and requirements:
For general use and aesthetics: S355J0W is often the standard and most readily available choice for buildings, sculptures, and containers where very low temperatures are not a concern.
For critical structures or cold climates: If your project is a bridge, a load-bearing frame in a region with cold winters, or any safety-critical structure, specifying S355J2W or S355K2W provides verified toughness against brittle fracture.
Always verify with mill certificates: For structural integrity, always require the material's mill test certificate. This document verifies that the delivered plate meets the required mechanical and chemical properties for your specified grade.

In summary, S355W Corten steel provides a minimum yield strength starting at 355 MPa and a tensile strength between 470-630 MPa. By understanding the nuances behind its name and related grades like S355J2W, you can make an informed selection that ensures both durability and structural safety for your specific application.