What is A588GrA weathering steel Plates

Sep 04, 2025 Leave a message

A588 Grade A Atmospheric Corrosion Resistant Steel Description

 

A588 Grade A steel plate is for high strength low alloy structural steel with 345Mpa minimum yield point to 100mm thickness. When properly exposed to the atmosphere, A588 Grade A is suitable for many applications in the bare condition.

 

Equal steel grade of ASTM A588 Grade A, in other standards: EN 10155 :S355J2G1W;SEW 087:WTSt 52-3; UNI: Fe510 D2K1; BS 4360: WR 50 C and some other steel grade.

 

A588 Grade A Steel Delivery Conditions

 

Hot Rolled, Cold Rolled, Normalized, Quenched, Tempering, Thermal Mechanical Control Process (TMCP), Electroslag Remelting Technical, HIC test.

 

A588 Grade A Steel Application

 

The atmospheric corrosion resistance of A588 Grade A steel in most environments is substantially better than that of carbon structural steels with or without copper addition. When properly exposed to the atmosphere, A588 Grade A steel is suitable for many applications in the bare (unpainted) condition.

A588 Grade A

 

ASTM A588 Grade A Atmospheric Corrosion Resistant Steel is used for various types of welded, bolted and riveted constructions e.g. steel frame structures, bridges, tanks and containers, exhaust systems, vehicles and equipment constructions.

 

A588 Grade A steel Chemical Composition Analysis

 

Carbon, % Manganese, % Cr % Silicon % N % max Sulfur %
Max 0.19 0.80-1.25 0.40-0.65 0.30-0.65 0.010 0.040
Cu % Phosphorus % Ni % Mo %    
0.25-0.40 0.05 0.40 ….    

 

A588 Grade A steel Mechanical Properties

 

Thickness Yield Strength
ReH[N/mm2]transv.min
TensileStrength
Rm[N/mm2]transv
Fracture Elongation[%]transv. min. Notch ImpactEnergy1)Ch Vcomplete samplelongitud. min [J]
0mm-100mm 340 KPa 480 KPa - - -
102mm-127mm 320 KPa 460 KPa      
127mm-203mm 290 KPa 430 KPa      

 

A588 Grade A Steel Services

 

Pretreatment(Derusting,Lacquering,Painting,Sand Clusting),Heat treatment,UT Test,HIC Test,Impact Test,PWHT Z15 Test, Z25 Test, Z35Test,Cutting, Welding ,Inspection from the third party like SGS,Galvanization

 

ASTM A588 Grade A steel plate/weathering steel/corrosion resistant/weather resistant steel: Gnee can supply the stock steel grade A588 Grade A Weathering Steel, Gnee Steel is a professional A588 Grade A steel plates exporter,supplier,manufacturer and stockist in China.

 

A588 Grade A

 

Any need in A588 Grade A Weathering Steel,please feel free to contact us! We will offer you the most competitive price of A588 Grade A and best service for A588 Grade A.

Contact now to get A588 Grade A Quote