What is ASTM A 709 Gr.50W weathering steel plate,

Sep 04, 2025 Leave a message

A 709 Gr.50W Weathering Steel Description

 

ASTM A709 Grade 50W equal grade are EN10155 :S355K2G1W,NFA 35-502,E 36 WB 4 .A709 Grade 50W is the specification used for steel plate used in the manufacture of bridges.

A709 Grade 50W

 

A 709 Gr50W Weathering Steel Delivery Conditions

 

Hot rolled,Cold rolled,Normalization,Tempering,Quenched,Normalization and Tempering,Quenched and Tempering,UT,PWHT,IMPACT TEST,Thermal Mechanical Control Process (TMCP),Electroslag Remelting Technical,HIC test,etc.

 

A 709 Gr50W Weathering Steel Applications

 

gnee Steel stocks A709 Grade 50W. These grades are often specified with charpy tests referencing the specific zone (or climatic region) in which the bridge will be in use.

A709 Grade 50W

A709 Grade 50W is used for various types of welded, bolted and riveted constructions e.g. steel frame structures, bridges, tanks and containers, exhaust systems, vehicles and equipment constructions.

 

A 709 Gr.50W Weathering Steel Chemical Composition

 

Steel Grades C
max
Si
max
Mn P
max
S
max
Cu
max
Cr
max
Ni
max
V
max
Nb
max
Al
min
A 709 Gr.50W - - - 0.035 0.035 - - - - - 0.020

 

 

 

 

 

A 709 Gr.50W Weathering Steel Mechanical properties

 

A709 Grade Thick
mm
Yield
[MPa]
Tensile [MPa] Elongtation Min % reduction
Min
%
HB
Steel Plate Structural steel
8in[200mm] 2in[50mm] 8in[200mm] 2in[50mm]
50W[345W]
HPS50W[HPS345W]
≤100 345min 485min 18 21 18 21J …  

 

A 709 Gr.50W Weathering Steel Services

 

Pretreatment(Derusting,Lacquering,Painting,Sand Clusting), Heat treatment,UT Test,HIC Test,Impact Test,PWHT Z15 Test, Z25 Test, Z35Test,Cutting, Welding ,Inspection from the third party like SGS,Galvanization

 

ASTM A 709 Gr.50W steel plate/weathering steel/corrosion resistant/weather resistant steel: Gnee can supply the stock steel grade A 709 Grade50W Weathering Steel, Gnee Steel is a professional weathering steel exporter,supplier,manufacturer and stockist in China.

 

Any need in A 709 Grade50W Weathering Steel, please feel free to contact us! We will offer you the most competitive price of A 709 Gr.50W and best service for A 709 Gr.50W.

Contact now to get A 709 Gr.50W Quote