FE 510 D1K1 Steel Description
FE 510 D1K1 steel grade is a hot rolled products of structural steels in technical delivery conditions with improved atmospheric corrosion resistance.The main alloying elements are chromium nickel and copper with added phosphorous which gives it excellent self protecting qualities.
As the steel reacts with elements in the atmosphere, the material forms a layer of rust over time which in essence protects the steel from corrosion.
FE 510 D1K1 steel is the Equivalent grades as S355J2WP (1.8946) steel in EN 10025 - 5 : 2004 standard and A242 Type1 steel in ASTM standard and also E36WA4 steel in NFA 35-502 standard.

FE 510 D1K1 Steel Delivery state
Hot Rolled, Cold Rolled, Normalized, Quenched, Tempering, Thermal Mechanical Control Process (TMCP), Electroslag Remelting Technical, HIC test.
FE 510 D1K1 Steel Application
Corrosion resistant steel plate FE 510 D1K1 under standard UNI is mainly used for container steel.
Moreover, FE 510 D1K1 steel with improved atmospheric corrosion resistance has a wide range of applications: architecture, smokestacks, fabrication,freight wagons, silos, pylons and bridges.
FE 510 D1K1 steel alloying with copper and chromium ensure the formation of a firmly adhering protective layer of rust which concurrently makes for an attractive appearance.

FE 510 D1K1 Steel Chemical Composition
| C % | Mn % | Cr % | Si % | CEV % | S % |
| Max 0.12 | Max 1 | 0.3-1.25 | Max 0.75 | Max 0.52 | Max 0.03 |
| Cu % | P % | ||||
| 0.25-0.55 | 0.06 - 0.15 |
For long products the P and S content can be 0.005% higher
The FE 510 D1K1 steels may show a Ni content of max. 0,65 %
The FE 510 D1K1 steels shall contain at least one of the following elements: Al total ≥ 0,020 %, Nb: 0,015 - 0,060 %, V: 0,02 - 0,12 %, Ti: 0,02 - 0,10 %. If these elements are used in combination, at least one of them shall be present with the minimum content indicated.
FE 510 D1K1 Steel Mechanical Properties
| Grade | Min. Yield Strength Mpa | Tensile Strength MPa | Impact | ||||||||
| FE 510 D1K1 | Nominal Thickness (mm) | Nominal Thickness (mm) | degree | J | |||||||
| Thick mm | ≤16 | >16 ≤40 |
>40 ≤63 |
>63 ≤80 |
>80 ≤100 |
>100 ≤150 |
≤3 | >3 ≤100 | >100 ≤150 | -20 | 27 |
| FE 510 D1K1 | 355 | 345 | …. | …. | …. | …. | 510-680 | 470-630 | …. | ||
If FE 510 D1K1 mechanical properties have been significantly modified by heavy coldforming, either stress relief annealing or normalised may be applied.
Normalised should also be applied following hotforming outside of the temperature range of 750 - 1.050 °C and after overheating.
The tensile test values given in the table apply to longitudinal samples; in case of strip and sheet steel of widths of ≥600 mm they apply to transverse samples.
FE 510 D1K1 Steel Services
Cutting, Painting, shot blast, and The third party inspection in DNV, BV, LR, GL, ABS, CCS , SGS, and others in super thick ship steel plate.
Gnee Corten Steel is specialized in super thick atmospheric corrosion resistance of structural steel plate.
Bebon Internationl has very good relationship with every big steel mill, so we could promise the delivery time and the competitive price compared with other companies.
Besides that, Gnee Corten Steel is a professional FE 510 D1K1 steel exporter and a steel Stockist in china. We keep more than 1000 tons FE 510 D1K1 steel in stock every month. So, if you have any inquiry about FE 510 D1K1 steel, if you are looking for a sincerely FE 510 D1K1 steel supplier and want to get the FE 510 D1K1 steel price, please do not hesitate to contact us.
Any need in FE 510 D1K1 steel grade, please feel free to contact us by email or calling to us, we will supplier high quality FE 510 D1K1 steel with competitive price to you soon.
Contact now to get FE 510 D1K1 Quote