What is Fe 510 C2K1 High Strength Low Alloy Corten steel plate

Sep 08, 2025 Leave a message

 

Fe 510 C2K1 Steel Description

 

 

As a structural weathering steel, Fe 510 C2K1 steels have a super property. Fe 510 C2K1 steel chemical composition can increase resistance to atmospheric corrosion compared to other steels.

 

Fe 510 C2K1 steels

 

This is because it forms a protective layer on Fe 510 C2K1 steel surface under the influence of the weather.

 

 

Fe 510 C2K1 steel deliver condition

 

 

Hot Rolled, Cold Rolled, Normalized, Quenched, Tempering, Thermal Mechanical Control Process (TMCP), Electroslag Remelting Technical, HIC test.

 

 

Fe 510 C2K1 Steel Application

 

 

Fe 510 C2K1 steel steel is used for various types of welded, bolted and riveted constructions e.g. steel frame structures, bridges, tanks and containers, exhaust systems, vehicles and equipment constructions.

Fe 510 C2K1 steel steel

 

Fe 510 C2K1 steel chemical composition by [%]

 

 

C Si Mn P S Cr N Cu CEV
max 0.16 Max 0.5 0.5 - 1.5 max 0.035 Max 0.035 0.4 -0.8 max 0.009 0.25-0.55 Max 0.52

Note:
1. The steels may show a Ni content of max 0.65 %;


2. For long Fe 510 C2K1 steel, the P and S content can be 0.005% higher;


3. The Fe 510 C2K1 steel may contain max. 0.30 % Mo and max. 0.15 % Zr


4. It is permissible to exceed the specified values provided that for each increase of 0.001 % N, the P max. content will be reduced by 0.005 %; the N content of the ladle analysis, however, shall not be more than 0.012 %


5.The max. value for nitrogen does not apply if the chemical composition shows a minimum total Al content of 0.020 % or if sufficient other N binding elements are present.

 

 

Fe 510 C2K1 steel Mechanical properties

 

 

 

 

Nominal thickness (mm) to 16 16-40 40-63 63-80 80-100 100-150
ReH - Minimum yield strength (MPa) 355 345 335 325 315 295
Nominal thickness (mm) To 3 3-100 100-150
Rm -Tensile strength (MPa) 510-680 470-630 450-600
Nominal thickness (mm) 3-40 40-63 63-100 100-150
A - Minimum elongation Lo = 5,65 √ So (%) 22 21 20 18
Nominal thickness (mm) 1.5 - 2 2-2.5 2.5-3
A - Minimum elongation Lo = Lo = 80 mm (%) 16 17 18
Temperature -20 0
Notch impact test. Min. absorbed energy 27 27

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

Contact now to get Fe 510 C2K1 Quote

 