What is the equivalent of S355J0W atmospheric corrosion resistant steel sheet?

Oct 27, 2025 Leave a message

Products Description

S355J0W steel is a kind of weathering steel, also known as atmospheric corrosion resistant steel, is a low alloy steel series between ordinary steel and stainless steel.

 

This steel is made of ordinary carbon steel with a small amount of copper, nickel and other corrosion resistant elements, so that it has stronger weather resistance than ordinary steel.

 

S355J0W

 

In the grade representation of S355J0W steel, "S" stands for structural steel, "355" stands for the lowest yield strength of 355MPa when the thickness is less than or equal to 16mm, "J" stands for the quality identifier of the relevant impact work value, "0" stands for 0℃ impact test, and "W" stands for the resistance of steel to atmospheric corrosion. The standard of S355J0W steel plate is EN10025-5:2004.

 

Chemical Composition

 

Grade

C

Si

Mn

P

S

N

Addition of
nitrogen binding
elements

Cr

Cu

S355J0W

0.16

0.50

0.50/1.50

0.035

0.035

0.009

–

0.40/0.80

0.25/0.55

 

Mechanical Properties

 

Grade

Min. Yield Strength Reh MPa

Tensile Strength Rm MPa

Nominal Thickness (mm)

Nominal Thickness (mm)

≤16

>16 ≤40

>40 ≤63

>63 ≤80

>80 ≤100

>100 ≤150

>3

>3 ≤100

>100 ≤150

S355J0W

355

345

335

325

315

295

510/680

470/630

450/600

 

Grades & Equivalents

 

EN 10025-5:2004

Corten

S355J0W

Corten B

 

Products Application

 

S355J0W steel plate can be used for the manufacture of containers, rolling stock, oil derrick, harbor construction, oil platforms and chemical structure of petroleum equipment containing hydrogen sulfide and other corrosive medium container.

 

Contact now to get S355J0W Quote

 

info-612-706

 

FAQ

Q: What is the equivalent of S355J0W?

A: The equivalent grade of S355J0W under NFA 35-502 standard is E 36 WB 3. And S355J0W equivalent grade of BS4360 standard is WR 50 B. S355J0W equivalent grade of ISO 4952 standard is Fe 355 W.

Q: What is Characteristics of S355J0W steel?

A: Excellent atmospheric corrosion resistance: S355J0W steel adds a small amount of corrosion resistance elements such as copper and nickel on the basis of ordinary steel, which can form a dense protective film on the surface of the steel plate and effectively resist corrosion factors in the atmosphere, such as moisture, oxygen and pollutants. Therefore, the atmospheric corrosion resistance of S355J0W steel is 2 to 8 times that of ordinary carbon steel, and it has a long service life.