What is the yield strength of ASTM A606-2 weathering steel?

Feb 26, 2026 Leave a message

Minimum yield strength (2% offset):

Hot‑rolled plate/sheet (as‑rolled): 50 ksi (345 MPa)

Hot‑rolled (annealed/normalized): 45 ksi (310 MPa)

Cold‑rolled sheet/coil: 45 ksi (310 MPa)

info-381-271

 

The yield strength of ASTM A606-2 weathering steel varies slightly depending on its delivery condition (hot‑rolled, cold‑rolled, or heat‑treated), but it is classified as a high‑strength low‑alloy (HSLA) weathering steel with a well‑defined minimum yield strength.

 

For hot‑rolled sheet and plate in the as‑rolled condition, the minimum specified yield strength is 50 ksi (345 MPa). This is the most common and widely referenced value for structural and landscape applications.

info-308-263

For material supplied in cold‑rolled or annealed/normalized condition, the minimum yield strength is typically 45 ksi (310 MPa).

In all cases, the yield strength is significantly higher than that of ordinary mild carbon steel, which allows the use of thinner and lighter sections while maintaining structural safety and stability in outdoor landscape and architectural components.

 

This high yield strength is one of the key advantages of ASTM A606‑2, distinguishing it from lower‑strength weathering steels such as SPA‑C and making it suitable for load‑bearing exterior panels, retaining walls, landscape structures, and formed architectural elements.