A847 Grade Atmospheric Corrosion-Resistance Square Steel Pipe

A847 Grade Atmospheric Corrosion-Resistance Square Steel Pipe

ASTM A847 is a specification for high strength low alloy (HSLA) weathering steel cold-formed and welded into square and rectangular tubing and pipe.
Send Inquiry
Description
Technical Parameters

Products Description

 

ASTM A847 is a specification for high strength low alloy (HSLA) weathering steel cold-formed and welded into square and rectangular tubing and pipe.

 

A847 steel pipe and tube are widely used products which are ideal for atmospheric corrosion resistance and are generally left unpainted. Elements such as copper, chromium, nickel and silicon are used for enhanced corrosion resistance.

 

product-439-439

 

A847 is employed in applications where corrosion resistance is the critical factor and is widely used for fencing, signposts, and sign structures (highway DOT).

 

Its attractive finish makes it highly suitable for pedestrian bridges, highway bridges, outdoor pavilions, architectural exposed structural applications, and more.

 

Products specification

 

Sizes Thickness Grades
40*40 – 300*300 mm 1/8, 3/16, 1/4, 3/8, 1/2 inch Gr A & B
Specification Application End
ASTM A847 highway bridges plain, beveled end

 

Size Chart of corten square structural tubing

 

HEIGHT X WIDTH (MM) 12.5 MM (kg/m) 2.5 MM (kg/m) 2.0 MM (kg/m) 3.0 MM (kg/m) 5.0 MM (kg/m) 4.0 MM (kg/m) 6.0 MM (kg/m) 10.0 MM (kg/m) 8.0 MM (kg/m)
50 x 50 - 3.60 2.93 4.25 6.56 5.45 - - -
40 x 40 - 2.82 2.31 3.30 - 4.20 - - -
60 x 60 - 4.39 3.56 5.19 8.13 6.71 - - -
80 x 80 - - - 7.07 11.3 9.22 13.2 - -
70 x 70 - - - 6.13 9.70 7.97 - - -
90 x 90 - - - 8.01 12.8 10.5 15.1 - -
120 x 120 - - - - 17.6 14.3 20.8 31.8 26.4
140 x 140 - - - - 20.7 16.8 24.5 38.1 31.4
100 x 100 - - - 8.96 14.4 11.7 17.0 - 21.4
150 x 150 48.7 - - - 22.3 18.0 26.4 41.3 34.0
180 x 180 60.5 - - - 27.0 - 32.1 50.7 41.5
160 x 160 52.6 - - - 23.8 19.3 28.3 44.4 36.5
200 x 200 68.3 - - - 30.1 - 35.8 57.0 46.5
250 x 250 88.0 - - - - - 45.2 72.7 59.1
220 x 220 76.2 - - - - - 39.6 63.2 51.5
300 x 300 108 - - - - - 54.7 88.4 71.6

 

Yield/Tensile Strength

 

Metric

Imperial

Tensile Strength, Ultimate

483 MPa

70,000 ksi

Tensile Strength, Yield

345 MPa

50,000 ksi

Elongation at Break

(in 50 mm)

N/A

N/A

 

Material Chemistry

 

C

MN

P

S

CU

0.24% max

1.40% max

0.15% max

0.06% max

0.20%

 

STM A847 hss square tube chemical properties

 

IRSM 41 -97 ASTM 588 GR A Corten – A Plates ASTM 242 TYPE -1
Manganese 0.25-0.45 0.80-1.25 0.20-50 1.00
Carbon, Max 0.10 0.19 0.12 0.15
Phosphorus 0.07-0.11 0.04 0.07-0.15 0.15
Silicon 0.28-0.72 0.30-0.65 0.25-0.75 0.25-0.40
Aluminimum 0.030 … – –
Sulphur, max 0.030 0.05 0.030 0.05
Chromium 0.30-0.50 0.40-065 0.50-1.25 –
Nickel, max 0.20-0.49 0.40 0.65 –
Copper 0.30-0.39 0.25-0.40 0.25-0.55 0.20 min
Molybdenum, max – – – –
Vanadium 0.050 0.02-0.10 – –

 

Applications of ASTM A847 Weathering Steel Tube & Pipe

 

ASTM A847 weathering steel pipe and tube is designed for structural and architectural applications that require high strength and long-term resistance to atmospheric corrosion. It can be used bare (unpainted) for many outdoor installations, as it forms a stable, protective oxide layer that eliminates the need for painting or regular maintenance.

 

Typical applications include:


• Pedestrian bridges and highway bridges, where A847's minimum yield strength of 345 MPa and tensile strength up to 485–635 MPa provide strong load-bearing capability and long service life under varying weather conditions.


• Outdoor pavilions, architectural exposed structures, and landscape elements, where its natural rust-like patina blends beautifully with urban or natural surroundings.


• Fencing, guardrails, and guide rails, taking advantage of its durability and resistance to abrasion and oxidation.


• Sign posts, lighting poles, and street furniture, offering excellent mechanical strength and minimal maintenance over decades of outdoor exposure.


• Industrial and marine environments, such as pipe supports, walkways, and port structures, where resistance to humidity, salt air, and pollutants is essential.

 

Corten A847 tubes are available in round, square, and rectangular sections, typically in sizes ranging from ½ inch to 20 inches in diameter and wall thicknesses from 2 mm to 40 mm. These properties make A847 an ideal choice for modern architectural designs, infrastructure projects, and urban landscaping requiring both structural reliability and aesthetic appeal.

 

Contact now to get ASTM A847 Weathering Steel Tubing Quote

 

product-800-1000

Hot Tags: a847 grade atmospheric corrosion-resistance square steel pipe, China a847 grade atmospheric corrosion-resistance square steel pipe manufacturers, suppliers, welded Corten pipe, 09CrCuSb Seamless Corten Pipe, Welded Corten Steel Pipe, round corten tubing, corten steel square tube, Rectangular Corten Tube