S355J2W Corten Steel Pipes

S355J2W Corten Steel Pipes

Products Description S355J2W Corten Steel Pipe is a weather-resistant steel pipe known for its excellent impact strength, making it ideal for heavy-duty structures and low-temperature environments. The pipe is available in diameters ranging from 50mm to 1200mm, with wall thicknesses from 3mm to...
Send Inquiry
Description
Technical Parameters

Products Description

 

S355J2W Corten Steel Pipe

S355J2W Corten Steel Pipe is a weather-resistant steel pipe known for its excellent impact strength, making it ideal for heavy-duty structures and low-temperature environments.

 

The pipe is available in diameters ranging from 50mm to 1200mm, with wall thicknesses from 3mm to 40mm, and lengths typically between 6m and 12m, which can be customized according to project requirements.

 

Over time, the surface naturally develops a protective rust layer that effectively prevents further oxidation, eliminating the need for additional coatings or complex maintenance.

 

 

Specification

 

Size Range ½” OD to 16” OD
Standards ASTM A 423 GR. 1,ASME SA 423, ASTM A 847, ASTM 588, ASTM 606
Grade S355J2W Corten Steel Pipe
Shape Round, Square, Rectangle, Hydraulic, Honed Tubes
Length Single Random, Double Random & Cut Length
End Plain End, Beveled End
type Weathering steel / corten steel

 

S355J2W Corten Steel Pipe Grades & Equivalents

 

EN 10025-5:2004 CORTEN
S355J2W

 

Corten B

 

S355J2W Corten Steel Tube Mechanical Properties

 

GRADE MIN. YIELD STRENGTH REH MPA           TENSILE STRENGTH RM MPA    
  Nominal Thickness (mm)           Nominal Thickness (mm)    
  <16 >16 <40 >40 <63 >63 <80 >80 <100 >100 <150 >3 >3 <100 >100 <150
S355J2W 355 345 335 325 315 295 510/680 470/630 450/600

 

S355J2W Weathering Steel Chemical Composition

 

  %
C 0.16
Si 0.50
Mn 0.50/1.50
P 0.030
S 0.030
N 0.009
Cr 0.40/0.80
Cu 0.25/0.55

 

S355j2w Steel Pipe Weight

 

S355J2W Corten Pipe thickness DIN 1.8963 Pipe weight
(lbs/ft)
3/8″ 15.315
1/4″ 10.210
1/2″ 20.420

 

EN 10025 S355J2W Tubing Thermal Properties

 

Properties Conditions
T (°C)
Thermal Conductivity (W/m-K) 42.7 100
Specific Heat (J/kg-K) 477 50-100

 

Corten Steel EN 10025 S355j2w Steel Piping Equivalent Material

 

Grade DIN
S355J2W 1.8965

 

S355j2w Corten Steel Tube Physical Properties

 

Quantity Value Unit
Density 8000 kg/m3
Thermal expansion 16 – 17 e-6/K
Thermal conductivity 16 W/m.K
Service temperature 0 – 500 °C
Melting temperature 1370 – 1400 °C
Resistivity 0.7 – 0.7 Ohm.mm2/m
Specific heat 500 – 500 J/kg.K

 

About Us

 

At Gnee, we know how critical on-time delivery and quality consistency are. Our streamlined project management system ensures every order is traceable, transparent, and executed with precision from start to finish.

 

Our one-stop delivery service includes:

  • Clear production timeline and project planning
  • CNC machining with strict manual inspections
  • 100% final inspection before shipping with factory reports
  • Comprehensive export logistics and document support
  • Ongoing installation guidance and after-sales support

 

S355j2w Corten Steel

Hot Tags: s355j2w corten steel pipes, China s355j2w corten steel pipes manufacturers, suppliers, A847 Rectangular Corten Tube, Rust Resistant Welded Pipe, Sulfuric acid dew point Seamless pipe, weathering steel tube, Corten Rectangular Tube, weathering steel pipe