EN 10025 5 S355J2W N High Strength Weathering Steel Sheet

EN 10025 5 S355J2W N High Strength Weathering Steel Sheet

S355J2W N is a medium tensile, low carbon manganese weathering steel which is readily weldable and possesses good impact resistance, including in low temperatures. This material is commonly supplied in the untreated or normalized condition.
Send Inquiry
Description
Technical Parameters

Products Description

 

S355J2W N is a medium tensile, low carbon manganese weathering steel which is readily weldable and possesses good impact resistance, including in low temperatures. This material is commonly supplied in the untreated or normalized condition.

 

S355J2W

Products Specification

 

Grade : S355J2W+N Corten Steel Plates
Standard : ASTM A588, A242 / ASME SA588, SA242
Width : 750mm to 1500mm,
Length : 2500mm to 12000mm
Thickness : 3MM to 50mm
Type : Corten Steel / High-Strength Low-alloy Structural Steel
Process : Hot-Rolled (HR)

 

S355J2W+N Corten Steel Plates Chemical Composition

 

C Si Mn P S Cr Zr Ni Cu Mo CEV
0.16 max. 0.50 max. 0.50 max. 0.03 max. 0.03 max. 0.40-0.80 0.15 max. 0.65 max. 0.25-0.55 0.03 max. 0.44 max.

 

Corten Steel S355J2W+N Plates Mechanical Properties

 

Yield Strength Tensile Strength Minimum Elongation A (Lo = 5.65 vSo) %
355 MPa 510 - 680 MPa 20

 

S355J2W+N Corten Steel Plates Equivalent Grades

W. Nr. DIN EN BS JIS AFNOR USA
1.8965 WSt52.3 S355J2G1W
Fe510D2KI
WR50C SMA570W E36WB4 A588Gr.A
A600A
A600B
A600

 

Applications of S355J2W+N Corten Steel Plate

 

1. Transport Tanks
S355J2W+N Corten steel is widely used in the manufacturing of transport tanks for chemicals, petroleum, and other industrial liquids. Its superior atmospheric corrosion resistance minimizes maintenance requirements and ensures long-term protection against rust, even under harsh weather or outdoor exposure.

 

2. Steel Sculptured Buildings
Architects and designers favor S355J2W+N Corten steel for modern sculptural buildings and art installations. Its distinctive rust-like appearance evolves naturally over time, giving each structure a unique and enduring character while maintaining excellent structural integrity.

 

3. External Wall Claddings of Buildings
The steel's natural weathering property makes it an ideal choice for exterior wall claddings. It forms a stable oxide layer that protects the surface from further corrosion, eliminating the need for painting or coating. This makes it both cost-effective and visually striking for contemporary architectural facades.

 

4. Weather Strips
Due to its ability to withstand fluctuating climatic conditions, S355J2W+N steel is often used in weather strips and sealing applications. The material retains its strength and appearance despite exposure to moisture, UV radiation, and temperature changes.

 

5. Welded Structures
S355J2W+N grade steel offers excellent weldability, making it suitable for a variety of welded structures such as bridges, frameworks, and support systems. Its high yield strength and toughness provide durability and safety in demanding engineering environments.

 

 

6. Gas Flue and Aesthetic Facias
This steel is also employed in the fabrication of gas flue systems and building facias where both functionality and appearance are important. Its resistance to oxidation and its rich patina color contribute to both performance and architectural appeal.

 

7. Freight Containers
S355J2W+N Corten steel is frequently used in the production of freight containers and shipping units. Its corrosion-resistant surface ensures extended service life in marine and coastal conditions, reducing the need for maintenance and repainting over time.

 

Contact now to get S355J2W+N Quote

 

product-574-365

Hot Tags: en 10025 5 s355j2w n high strength weathering steel sheet, China en 10025 5 s355j2w n high strength weathering steel sheet manufacturers, suppliers, ASTM Corten Plate, Corten Steel Laser Cutting, perforated corten steel facade, weathering steel coil, Corten A Steel Coil, weathering steel plate