S355K2W weather resistant steel plate is a low-alloy structural steel grade under the European standard EN 10025-5, specially designed to resist atmospheric corrosion. It is widely used for outdoor structures and projects exposed to harsh environmental conditions.
Send Inquiry
Description
Technical Parameters

S355K2W weather resistant steel plate is a low-alloy structural steel grade under the European standard EN 10025-5, specially designed to resist atmospheric corrosion.

 

product-599-530

 

It is widely used for outdoor structures and projects exposed to harsh environmental conditions.

 

Features

 

 

product-547-543Excellent Weather Resistance
The S355K2W weather resistant steel plate forms a dense protective oxide layer (patina) when exposed to natural weather, effectively preventing further corrosion and extending the service life while reducing maintenance costs.

 

 

It is ideal for outdoor applications such as bridges, building facades, and industrial equipment.

 

High Strength
With a minimum yield strength of 355 MPa, this steel plate provides outstanding structural strength while maintaining good weldability and machinability.

 

Versatile Applications
Suitable for a wide range of uses including construction, bridges, sculptures, and industrial manufacturing.

 

Its excellent formability and weldability make it a favorite among engineers and designers.

 

 

product-568-561

Durability and Longevity
Its inherent corrosion resistance ensures long-term durability of structures, minimizing the need for frequent maintenance and repairs.

 

Compliance with Standards
Manufactured strictly according to EN 10025-5, ensuring consistent quality and performance in construction projects.

 

Sustainable and Environmentally Friendly
The natural protective patina eliminates the need for additional coatings or paints, reducing environmental impact and aligning with green building principles.

 

Aesthetic Appeal
The naturally weathered surface offers a unique, rustic look that blends harmoniously with natural surroundings, favored by architects and designers.

 

 

 

Specifications

 

 

product-546-549

 

Thickness Range: 2mm – 460mm

 

Width Range: 1500mm – 3200mm

 

Length Range: 6000mm – 12000mm

 

Equivalent Grade: E36WB4 (Germany WBL 087 standard)

 

 

 

 

 

Chemical Composition (%)

 

 

Element C Si Mn Cu P S Cr N
Content 0.19 0.55 0.45-1.60 0.20-0.60 0.035 0.035 0.35-0.85 0.010

 

 

Mechanical Properties

 

 

Thickness (mm) Min Yield Strength (MPa) Tensile Strength (MPa) Impact Test (-20°C, J)
≤16 355 470-630 40
16-40 345 470-630 40
40-100 335 450-600 40
>100 295 450-600 40

 

 

Heat Treatment Conditions

 

 

Hot Rolled

 

Controlled Rolled

 

Normalized

 

Quenched and Tempered

 

Cold Rolled

 

Applications

 

 

The S355K2W weather resistant steel plate is widely used in bridge construction, outdoor sculptures, architectural facades, industrial equipment, and other outdoor structures requiring excellent corrosion resistance and high strength.

 

product-940-626

 

Supply and Service

 

 

As a professional S355K2W weather resistant steel plate supplier, we guarantee qualified products with timely delivery and competitive prices.

 

For inquiries about S355K2W steel plate price or technical specifications, please feel free to contact us for professional assistance and support.

Contact now

 

 

Hot Tags: hot rolled weather resistant s355k2w corten steel plate, China hot rolled weather resistant s355k2w corten steel plate manufacturers, suppliers, A588 steel sheet, Corrosion Resistance Corten Steel Coil, High Tensile Weathering Steel, plate corten, Pre treated Rusty Steel Plate, weathering steel sheet