A423 Gr 1 Coten Steel Heat-Exchanger and Condenser Tubes

Oct 13, 2025 Leave a message

Products Description

 

Corten Steel ASTM A423 Gr 1 Seamless Pipe eventually decreases and from that point on the finish acts as a protective coating for the base metal. This protective coating essentially stops the corrosion.

Corten Steel ASTM A423 Gr 1 Seamless Pipe

Laboratory analysis of the rust film have shown that the alloying elements in the steel, particularly copper, chromium, and nickel produced insoluble compounds that clogged the pores at the rust/steel interface, thereby ending the regeneration.

 

Product Features

 

Corrosion resistant

Accurate dimensions

Can sustain high pressure & temperature load

Rust proof finish

Smooth transition from flange thickness to pipe

Ensure excellent stress distribution

 

ASTM A423 Gr. 1 Heat Exchanger / Condenser Tubes Chemical Composition

 

Element A423 Gr. 1
C 0.15 Max
Mn 0.55 Max
P 0.06–0.16
S 0.060 max
Si 0.10 Min
Cu 0.20–0.60
Cr 0.24–1.31
Ni 0.20–0.70

 

A423 Gr 1 Corten Steel Heat Exchanger & Condenser Tubing Mechanical Properties

 

Element A423 Grade 1
Tensile Strength KSI (MPa) ≥415
Yield Strength KSI (MPa) ≥255
Elongation min. % ≥30

 

Corten Steel A423 / SA423 Gr 1 Heat Exchanger and Condenser Tube Application

 

Air Preheater Unit
Steam generating Boiler
Power Generation
Economiser
Heat Exchangers
Electric Power Plants
Fossil Fuel Plants
Water Supply Systems
Waste Heat Plants
Cogeneration Facilities

 

Contact now to get A423 Gr 1 Quote

 

info-536-393