Gnee, as a trusted steel supplier, offers A588 Grade A (Gr A) weathering, corrosion-resistant steel plates in China, providing competitive prices, full specifications, sizes, and detailed application guidance.
A588 Grade A steel sheet exhibits outstanding resistance to atmospheric corrosion, far exceeding ordinary carbon steel. This performance is due to the formation of a protective oxide layer on the surface, which slows further corrosion.
Both A588 Grade A and other weathering steels are high-strength, low-alloy materials, with a minimum yield strength of 50 ksi (345 MPa), allowing lighter structural designs and cost savings.

Primarily intended for unpainted applications, these steels reduce maintenance requirements such as repainting. Since its introduction, ASTM A588 Grade A has been widely used in bridges, rail cars, cranes, transmission towers, highway poles, chemical plants, factories, and shipbuilding.
Compared with conventional carbon steels like A36 and A572-50, A588 Grade A provides superior atmospheric corrosion resistance, with or without copper addition. Its minimum tensile strength is 70 ksi (483 MPa), suitable for heavy-duty structural applications.
Mechanical Properties
| Property | Metric | Imperial |
|---|---|---|
| Minimum Yield Strength | 345 MPa | 50 ksi |
| Minimum Tensile Strength | 483 MPa | 70 ksi |
| Elongation at Break (200 mm) | 20% | 20% |
| Elongation at Break (50 mm) | 23% | 23% |
| Modulus of Elasticity | 200 GPa | 29,000 ksi |
Chemical Composition (Grade A)
| Element | C | Mn | P | S | Si | Cr | Ni | Cu | V |
|---|---|---|---|---|---|---|---|---|---|
| Content | 0.19% | 0.80–1.25% | 0.03% | 0.03% | 0.03–0.65% | 0.40–0.65% | 0.40% | 0.25–0.40% | 0.02–0.10% |
Applications
| Field | Example Uses |
|---|---|
| Structural | Bridges, cranes, transmission towers, highway poles |
| Industrial | Chemical plants, factories, tanks, containers |
| Transportation | Rail cars, heavy equipment, shipbuilding |
As a reliable A588 Grade A steel supplier in China, Gnee provides stock availability, flexible sizes, and technical support. For inquiries about ASTM A588 Grade A steel, please contact us for the latest price, availability, or detailed specifications.