ASTM A709 Grade 50 Structural Steel Plate for Bridges
ASTM A709 Grade 50 is the workhorse bridge plate in the A709 family. It is a high-strength low-alloy steel with a minimum yield strength of 345 MPa, equivalent to 50 ksi, and it is stocked as heavy plate for girders, deck plates and supports. Certified mill test reports confirm both the mechanical properties and the chemical limits before a plate leaves the works.
Because bridges combine static loading, fatigue cycles and low service temperatures, Grade 50 is normally ordered with a minimum Charpy V-notch energy agreed for the climate and the position of the member in the structure.
Mechanical Properties
| Property | Imperial | Metric |
| Yield strength, Grade 36 | 36 ksi min | 250 MPa min |
| Yield strength, Grade 50 | 50 ksi min | 345 MPa min |
| Tensile strength, Grade 36 | 58-80 ksi | 400-550 MPa |
| Tensile strength, Grade 50 | 65 ksi min | 450-650 MPa |
| Elongation in 8 in (Grade 36) | 20 % min | 18 % min |
| Elongation in 8 in (Grade 50) | 18 % min | 18 % min |
The imperial and metric columns describe the same requirements. Design offices working in ksi specify 50 ksi minimum yield and 65 ksi minimum tensile; a mill test report written in metric units states 345 MPa and 450 MPa for the same plate.
Chemical Composition by Grade
| Grade | C max | Mn | P max | S max | Si | Other |
| ASTM A709 Grade 36 | 0.26 | 0.80-1.35 | 0.040 | 0.050 | 0.15-0.40 | Cu 0.20 min |
| ASTM A709 Grade 50 up to 4 in | 0.23 | 1.35 max | 0.030 | 0.030 | 0.15-0.40 | Cu 0.20 min where copper-bearing, Cb 0.005-0.15, V 0.01-0.15 |
| ASTM A709 Grade 50W Type A | 0.19 | 0.80-1.25 | 0.030 | 0.030 | 0.30-0.65 | Cu 0.25-0.40, Ni 0.40 max, Cr 0.40-0.65, V 0.02-0.10 |
| ASTM A709 Grade 50W Type B | 0.20 | 0.75-1.35 | 0.030 | 0.030 | 0.015-0.50 | Cu 0.20-0.40, Ni 0.50 max, Cr 0.40-0.70, V 0.01-0.10 |
| ASTM A709 HPS 50W and HPS 70W | 0.11 | 1.10-1.50 | 0.020 | 0.006 | 0.30-0.50 | Cu 0.25-0.40, Ni 0.25-0.40, Cr 0.45-0.70, Mo 0.02-0.08, V 0.04-0.08, Al 0.010-0.040, N 0.015 max |
Values are percentages by mass and are checked against the thickness of the order, because the limits for plate are tighter than those applied to rolled shapes. The microalloying package in the high-performance grades, molybdenum with vanadium, aluminium and nitrogen control, is what makes their toughness repeatable at low temperature.
A709 Grade 50 versus A572 Grade 50
| Point of comparison | ASTM A572 Grade 50 | ASTM A709 Grade 50 |
| General use | Buildings, transmission towers, equipment and general fabrication | Bridge members and similar structures needing toughness and weldability |
| Toughness | Not specified for bridge service | Charpy V-notch energy agreed for the zone and service temperature |
| Bridge recognition | Not a bridge specification | Dual certification with AASHTO M270 available |
| Yield strength | 345 MPa min | 345 MPa min |
The two grades share a 345 MPa minimum yield strength, so the choice is driven by the structure rather than by strength: A709 Grade 50 is the specification written for bridge use, with impact testing and certificate traceability built into the order.
Applications and Heavy Plate Supply
Bridge construction and long-span structures, including girders, webs and deck plates
Marine and shipbuilding work, especially the 50W, HPS 50W and HPS 70W weathering grades
Industrial plant and construction machinery subject to repeated loading
Structural components exposed to harsh environments, where toughness at low temperature matters
Plate is available in heavy thicknesses, with material 3 inches and thicker normally held at distribution centres so that bridge fabricators can be served without long rolling lead times. Plates can be supplied cut, drilled and edge-prepared to drawings, with dual ASTM and AASHTO certificates and impact test results reported per heat.
Frequently Asked Questions
Q: What is the yield strength of ASTM A709 Grade 50?
The specification requires a minimum yield strength of 50 ksi, which is 345 MPa, and Grade 50 plate is used for structural members in bridge building and similar structures.
Q: How does A709 Grade 50 differ from A572 Grade 50?
A572 Grade 50 covers general structural work such as buildings, towers and equipment. A709 Grade 50 is written for bridges and adds the toughness testing, weldability provisions and AASHTO M270 recognition that bridge owners require.
Q: What is the tensile strength of Grade 50 plate?
A minimum of 65 ksi, given in metric units as 450 MPa, with the permitted range extending to about 650 MPa depending on thickness and supply condition.
Q: Is A709 Grade 50 a weathering steel?
Not in itself. Grade 50W is the weathering version, which adds copper, chromium and nickel for atmospheric corrosion resistance; copper-bearing Grade 50 with 0.20 % minimum copper offers some additional resistance but is not the same material.
Q: What plate sizes are available?
Heavy plate with a minimum thickness from 5 mm up to 350 mm, widths from 900 mm to 4100 mm and lengths from 3000 mm to 25000 mm, with heavy plate 3 inches and thicker held in stock.
Q: Can Charpy impact testing be specified on the order?
Yes. Impact requirements are agreed for the specific zone and climate of the bridge, and the tested energy is reported on the mechanical certificate for each heat.