1. Limited Applicable High-Temperature Range
Cold-rolled SPA-H is not designed for long-term high-temperature service and is only suitable for short-term or intermittent use at ≤200℃ in ambient atmospheric conditions. For long-term continuous operation, the safe temperature limit is strictly ≤150℃, beyond which its performance degrades significantly.

2. Performance Degradation at Excessive Temperatures (>200℃)
Elevated temperatures above 200℃ will cause the work-hardened microstructure of cold-rolled SPA-H to undergo recovery and recrystallization, leading to a sharp drop in yield/tensile strength and hardness (losing the core advantage of cold-rolled strengthening). Meanwhile, ductility will recover but become unstable, and the steel's structural rigidity and load-bearing capacity will be severely reduced.

3. Impaired Corrosion Resistance in High-Temperature & Humid/Oxidizing Environments
At temperatures >200℃, especially in humid, high-oxygen or corrosive atmospheres, the protective patina of cold-rolled SPA-H cannot form stably and will oxidize rapidly to form loose, non-protective iron oxide. This accelerates atmospheric corrosion and even causes intergranular oxidation, completely losing the steel's inherent weathering performance.

4. Prohibited Use in Severe High-Temperature Scenarios
Cold-rolled SPA-H is strictly prohibited for use in environments with temperatures >300℃, as well as high-temperature cyclic heating/cooling, high-temperature load-bearing, and high-temperature corrosive (e.g., acid/alkali vapor) scenarios. At these temperatures, the steel will experience permanent microstructure damage, thermal deformation, and even brittle fracture, posing serious safety risks.