What ASTM A709 Grade 50W Covers

ASTM A709 is the specification for structural steel for bridges, and the 50W suffix identifies the weathering grade with a minimum yield strength of 50 ksi, roughly 345 MPa. Grade 50W is produced to a weathering chemistry similar to ASTM A588: copper with chromium and nickel additions that allow the exposed surface to develop a stable oxide layer instead of needing a protective coating system on every accessible face.

The grade is used where a bridge is designed as uncoated weathering steel, a common approach for highway structures in rural and moderately industrial atmospheres, and also where the steel is painted but a longer coating life is wanted. It is available in the same product forms as ordinary bridge plate, including as-rolled, normalized and quenched and tempered conditions depending on thickness and toughness requirements.

Chemistry and Mechanical Properties

Grade 50W is a copper-bearing low-alloy steel with chromium and nickel additions; the balance is controlled to keep carbon equivalent within a range suitable for welding, with carbon typically held at or below 0.19 per cent.

Property Value
Minimum yield strength 345 MPa (50 ksi)
Tensile strength 485 MPa (70 ksi) minimum
Minimum elongation 21 per cent in a 50 mm gauge length (plates)
Typical density 7.85 g/cm3
Modulus of elasticity 200 GPa (shear modulus approx. 80 GPa)
Melting range approx. 870-925 deg C (1600-1700 deg F)
Specific heat approx. 0.475 J/g deg C (0.105 Btu/lb deg F)
Practical maximum service temperature approx. 590 deg C (1100 deg F)

The combination of 345 MPa yield and a 485 MPa minimum tensile strength matches the design assumptions used in AASHTO load and resistance factor design, so grade 50W can be substituted directly for plain Grade 50 in a strength check without altering girder geometry. Heat treatment and toughness requirements are specified by thickness and by the fracture-critical designation of the member.

Bridge Applications and Fabrication Practice

Plate girders and rolled beams for highway and railway bridges, including curved and skewed spans.

Diaphragms, cross frames, splice plates and bearing stiffeners.

Exposed architectural steelwork on bridge parapets, railings and approach structures.

Fabrication follows normal bridge shop practice with two additions. Welding consumables must match the weathering chemistry so the weld metal develops a similar oxide to the parent plate; a copper-chromium-nickel filler of ER80S-G type or a low-hydrogen electrode of similar analysis is the usual choice, with heat input controlled to protect the heat-affected zone toughness. Second, fasteners and appurtenances should be stainless or weathering-grade, because plain carbon steel bolts or temporary attachments leave streaks that never disappear. In uncoated weathering design, longitudinal welds are made continuous where water can run, and details that would trap water or debris are revised at the drawing stage.

Size Range, Delivery Condition and Marking

Plate is supplied hot rolled in thicknesses from approximately 5 mm to 150 mm, with widths typically 1500-2500 mm and lengths up to 12000 mm; heavier and wider formats are available on a project basis. Deliverable finishes include as-rolled natural surface, black painted, shop-primed, blast cleaned with a holding primer, or oiled and varnished for transit protection. Each plate is marked with the grade, heat number, size and manufacturer identification, and stencilled or stamped markings are positioned so they do not remain visible on an uncoated architectural face.

Documentation normally comprises an EN 10204 type 3.1 inspection certificate with ladle analysis, tensile, yield and elongation results, charpy impact values where specified, dimensional tolerances referenced to ASTM A6, and ultrasonic examination results if ordered. Certification is traceable to the individual heat and, where required, to the plate number.

Quality Control, Corrosion Allowance and Long-Term Performance

For an uncoated weathering design, durability is handled as a corrosion allowance rather than by a coating. Loss rates are estimated from the site corrosivity category using ISO 9223 and from atmospheric exposure data, then applied as a sacrificial thickness over the design life, with additional allowance where runoff, ponding or chloride deposition is expected. The details that decide performance are the same ones that matter in any weathering structure: free drainage, no crevices, no contact with carbon steel and no permanently damp surfaces. Inspection in service consists of visual survey and periodic ultrasonic thickness readings at representative locations, typically at decade intervals, rather than repainting cycles. Field repairs are normally welded with matched consumables and dressed so that the repair patinates at the same rate as the surrounding steel.

Frequently Asked Questions

Q: What is the difference between ASTM A709 Grade 50 and Grade 50W?

A: Grade 50 is the plain high-strength low-alloy bridge grade, while 50W is the weathering version with copper, chromium and nickel additions. Both have a minimum yield strength of 345 MPa and a minimum tensile strength of 485 MPa, so 50W can replace Grade 50 in a strength check without changing the section.

Q: Can Grade 50W be used without any paint?

A: Yes, where the structure is designed as uncoated weathering steel. That requires free drainage, detailing that avoids crevices and ponded water, and a corrosion allowance based on the site corrosivity category rather than an assumption of zero loss.

Q: What thickness range is available?

A: Hot rolled plate is normally produced from about 5 mm to 150 mm thick in widths of roughly 1500-2500 mm and lengths up to 12000 mm, with heavier sections and cut-to-length plates supplied against project drawings.

Q: Which welding consumables should be used?

A: Filler metals with a matched weathering chemistry, such as a copper-chromium-nickel type ER80S-G classification for gas metal arc welding or a low-hydrogen electrode of similar analysis for manual metal arc welding, with heat input controlled to preserve toughness in the heat-affected zone.

Q: Is Grade 50W suitable for coastal bridges?

A: It can be used, but high chloride loading extends the time needed for a protective oxide to stabilise and increases pitting risk in splash and spray zones. Many coastal structures therefore combine weathering steel in the main span with coated steel or a coating system in the zones exposed to salt.

Q: What documentation accompanies a plate order?

A: An EN 10204 type 3.1 inspection certificate reporting ladle analysis and mechanical test results for each heat, dimensional tolerances to ASTM A6, and any specified non-destructive examination results, all traceable to the heat and plate number.