How to choose High Quality Corrugated Corten Steel.

Feb 02, 2026 Leave a message

Looking for high-quality corten steel corrugated panels for roofing or siding? GNEE is your trusted manufacturer, offering customized corten corrugated sheets in various sizes, thicknesses, and finishes.

 

corten steel corrugated panels

corten steel corrugated panels

 

Our panels are designed for durability, aesthetic appeal, and ease of installation. With GNEE, you can ensure fast delivery, superior quality, and professional service.

 

What is Corrugated Corten Steel?

 

Corrugated corten steel refers to corten sheets shaped in a wavy or corrugated pattern. This pattern provides additional structural strength, making it ideal for both roofing and siding applications.

 

Corten steel develops a protective rust-like patina when exposed to weather, which prevents further corrosion and enhances durability.

 

Applications include:

  • Roofing
  • Siding and cladding
  • Architectural and landscaping projects
  • Industrial and agricultural buildings

Corrugated corten steel combines rust-resistant properties with visual appeal, making it suitable for both exterior and interior designs.

 

GNEE Corten Advantages

 

Our gnee corten steel corrugated panel offer the benefits of corten steel without the downsides of natural rusting:

  • Arrives pre-weathered, no need to wait for rust formation.
  • No rust runoff or staining.
  • Comes with a standard paint warranty, unlike raw corten steel.
  • Suitable for exterior or interior applications.
  • Reduces pre-treatment time and costs compared to traditional corten steel.

Recommendation: Request a 7/8" corrugated sample panel to see the authentic finish up close.

 

Product Specifications

 

Property Details
Material Type 7/8" Corrugated Metal Roofing & Siding
Rib Distance (Pitch) 2.67"
Rib Height 7/8"
Available Gauges 22, 24
Fasteners Exposed
Panel Length 1' to 52' (customizable)
Recommended Min Roof Slope 3/12
Installation Over open purlin system or solid substrate; use bead mastic for roofing overlaps
Overall Width 39" (out-to-out, may vary by coil)
Roof Coverage 34.67"
Wall Coverage 37"
Substrate AZ50 Minimum (Galvalume®/Zincalume®)
Finish PVDF Resin-Based

 

Sizes and Weight

 

Size (mm) Weight per Panel Application
3000 x 1110 15 kg Roofing / Siding
Custom sizes available Based on length & thickness Roof & Wall panels

Other panel specifications:

Rib height: 7/8" (customizable)

Length: cut-to-order

Roof slope minimum: 3/12

 

Corten Corrugated Steel Mechanical & Chemical Properties

 

Equivalent Standards

Region Standard Grade
USA ASTM A588 GR. A, COR-TEN A, ASTM 242 TYPE-1
UK BS BS-6323-5, BS-6323-6
Germany DIN DIN 17177, EN10217-1/2
Japan JIS JIS G3445

Mechanical Properties

Steel Grade Yield Strength (MPa) Tensile Strength (MPa) Elongation (%)
ASTM 588 GR. A 345 485 21%
COR-TEN A 355 470–630 20%
ASTM 242 TYPE-1 345 480 16%

 

Chemical Composition (Max %)

Element ASTM 588 GR A IRSM 41-97 COR-TEN A ASTM 242 TYPE-1
C 0.19 0.10 0.12 0.15
Mn 0.80–1.25 0.25–0.45 0.20–0.50 1.00
P 0.04 0.07–0.11 0.07–0.15 0.15
S 0.05 0.030 0.030 0.05
Si 0.30–0.65 0.28–0.72 0.25–0.75 0.25–0.40
Cr 0.40–0.65 0.30–0.50 0.50–1.25 –
Ni 0.40 0.20–0.49 0.65 –
Cu 0.25–0.40 0.30–0.39 0.25–0.55 0.20 min
V 0.02–0.10 0.050 – –

 

Installation Techniques for Corten Corrugated Panels

 

Plan panel layout and direction of corrugations.

Secure panels with appropriate fasteners.

Overlap panels horizontally & vertically for water shedding.

Cut panels to size with proper tools; trim edges.

Install ridge caps and flashing for weather protection.

Allow space for thermal expansion and contraction.

Apply weatherproof sealant at edges & connections.

 

corten Corrugated Roofing vs Fencing

 

Feature Roofing Panels Fencing Panels
Purpose Roof coverage Privacy, security, decoration
Pattern Corrugated Various decorative
Size & Thickness Larger & thicker for load bearing Smaller & thinner
Installation Overlapping panels Mounted to posts
Maintenance Lower Higher

 

Pricing Factors for Corten Corrugated Steel

 

Larger orders may reduce per-unit cost.

Panel thickness and dimensions affect price.

Custom shapes and designs may increase cost.

Supplier reputation and location impact shipping & handling.

Market demand & availability influence material cost.

 

Testing & Quality Criteria

 

Corten corrugated panels are tested for:

Weather resistance & durability

Corrosion resistance

Load-bearing capacity

Water penetration prevention

Thermal expansion & contraction behavior

Impact & deformation resistance

Structural integrity of corrugations

 

Why Choose GNEE Corrugated Corten Panels?

 

Factory direct supply with fast delivery.

Custom sizes for roofing and siding.

Professional service & technical support.

Durable PVDF finish & AZ50 substrate for long-term performance.

Complete stock and made-to-order flexibility.

 

Contact us for the latest GNEE Corten Corrugated Steel panel price list. Ensure your roofing or siding project is completed with high-quality, rust-resistant, and aesthetically appealing corten steel panels.

 

Contact us for the latest GNEE 7/8" Corrugated Corten price list

 

info-500-510

 

Is corten steel cladding expensive?

Because of its high-strength, low-alloy composition and added durability, Corten Steel Cladding typically costs more upfront than mild steel or standard cladding materials. Prices can range from $600 to $1,200 per tonne, depending on material thickness, finishes, and supplier

 

What is a corten panel?

Corten Steel (sometimes known as weathered steel) is a group of steel alloys that are often used in outdoor construction. Corten Steel was designed to eliminate the need for painting and if left outside, exposed to the elements, they will develop a rusted appearance in just a few months.

 

What is the lifespan of corten steel?

Corten Steel thicknesses of modest specification [2.0mm or 3.0mm] are perfectly fit-for-purpose for + 25 years longevity, in most environments / applications. For + 40 years longevity, an additional 1.0mm thickness should be added, to mitigate the forecast material loss.

 

How thick are Corten panels?

The Corten is available in thicknesses from 22 gauge up to ½" thick in a variety of lengths and widths, which makes it compatible with any type of project.

 

Do magnets stick to corten steel?

Other than austenitic stainless steels, most steel does attract magnets. Galvanised steel, Corten steel, mild steel, cold-reduced steel and hot-rolled steel are all magnetic.

 

Can you seal Corten steel?

Everbrite Coating is a popular choice for sealing and protecting Corten steel to protect the rusted patina. It also prevents rust drips and staining problems by sealing in the rust patina, protecting the surrounding areas and people who may brush against the rust.