JIS G3114 SMA 50 CP atmospheric corrosion resistant steel Plate

Sep 04, 2025 Leave a message

SMA 50 CP Steel Description

 

SMA 50 CP steel is a structural weathering steel which is also referred to as atmospheric corrosion resistant steel. The main alloying elements are chromium nickel and copper with added phosphorous which gives it excellent self protecting qualities.

 

JIS G3114 SMA 50 CP atmospheric corrosion resistant steel Plate

 

As the steel reacts with elements in the atmosphere, the material forms a layer of rust over time which in essence protects the steel from corrosion

 

SMA 50 CP steel Deliver condition

 

Hot Rolled, Cold Rolled, Normalized, Quenched, Tempering, Thermal Mechanical Control Process (TMCP), Electroslag Remelting Technical, HIC test.

 

SMA 50 CP steel application

 

SMA 50 CP weathering steel has a widely use in Mine fans, earth moving buckets, trailers and large road vehicles, drill rings, cranes, excavators, underground mining equipment, bridges and other high strength components requiring superior toughness.

 

SMA 50 CP Corten Plate

 

SMA 50 CP steel chemical composition by [%]

 

C

Si

Mn

P

S

Cu

Cr

Ni

V

Nb

Al

Max 0.16

Max
0.50

Max
0.50-1.50

Max
0.035

Max
0.035

Max
0.25-0.55

Max
0.40-0.80

Max
0.65

Max
0.02-0.12

Max
0.015-0.060

Min
0.02

 

 

 

 

SMA 50 CP steel Mechanical properties

 

Thickness Yield Strength
ReH[N/mm2]
transv.min
Tensile
Strength
Rm[N/mm2]transv
Fracture Elongation[%]transv. min. Notch Impact
Energy1)Ch Vcomplete samplelongitud. min [J]
---- 355 510-610 22 ----

 

 

 

 

 

 

About Us

 

At Gnee, product safety is at the heart of everything we do. From raw materials to finished goods, we ensure every step in the production chain meets rigorous international safety standards.

 

Our Safety-Related Certifications Include:

 

ISO 45001:2018 Occupational Health & Safety Management
Guarantees a safe working environment in compliance with global safety practices.

 

EN 1090 + A1 CE Certification for Structural Steel
Ensures mechanical integrity and safety for demanding structural applications in the EU.

 

SGS / TUV / BV Mechanical Property Test Reports
Verifies yield strength, tensile strength, and impact resistance according to global safety norms.

 

MSDS (Material Safety Data Sheet) - Available upon request
Offers safety guidance for handling, transport, and storage of our steel products.

 

Gnee is committed to more than just high-performance steel - we deliver safe and dependable solutions for every project.

 

Contact now to get SMA 50 CP Quote

SMA 50 CP Corten Plate