WR 50 C steel description
As a structural weathering steel, WR 50 C steels have a super property. WR 50 C steel chemical composition can increase resistance to atmospheric corrosion compared to other steels.

This is because it forms a protective layer on WR 50 C steel surface under the influence of the weather.
WR 50 C steel deliver condition
Hot Rolled, Cold Rolled, Normalized, Quenched, Tempering, Thermal Mechanical Control Process (TMCP), Electroslag Remelting Technical, HIC test.
WR 50 C steel Application range
WR 50 C steel weathering steel has a widely use in Mine fans, earth moving buckets, trailers and large road vehicles, drill rings, cranes, excavators, underground mining equipment, bridges and other high strength components requiring superior toughness.

WR 50 C steel chemical composition(%)
|
C |
Si |
Mn |
P |
S |
Cu |
Cr |
Ni |
V |
Nb |
Al |
|
Max 0.16 |
Max |
Max |
Max |
Max |
Max |
Max |
Max |
Max |
Max |
Min |
WR 50 C steel mechanical property
| Thickness | Yield Strength ReH[N/mm2] transv.min |
Tensile Strength Rm[N/mm2]transv |
Fracture Elongation[%]transv. min. | Notch Impact Energy1)Ch Vcomplete samplelongitud. min [J] |
| ---- | 355 | 510-610 | 22 | ---- |
About Us
With robust R&D strength and flexible manufacturing systems, Gnee offers comprehensive OEM (Original Equipment Manufacturing) and ODM (Original Design Manufacturing) services to meet the diverse needs of global clients.
Our Services Include:
OEM Manufacturing – Mass production of weathering steel products under your brand with quality assurance.
ODM Design & Customization – Tailored services such as structural design, size customization, laser cutting, and surface treatment.
Rapid Prototyping – Quick sample development based on drawings or creative sketches to meet tight project timelines.
Whether you're a brand owner, designer, or contractor, Gnee is your reliable partner for high-quality, custom steel solutions.
Contact now to get Fe 510 C2K1 Quote