S355J0W Steel Plate is a common European standard heavy steel plate widely used in construction, bridges, engineering structures, and industrial fabrication projects.
The specification 80×2000×L indicates a thickness of 80mm, a width of 2000mm, and a customizable length according to project requirements.

S355J0W Steel Plate
With the continuous growth of global infrastructure and industrial development, the demand for S355J0W Weather Resistant Steel Plate is steadily increasing in the international steel market due to its excellent corrosion resistance, high strength, and low maintenance cost.
S355J0W Chemical Composition (%)
| Grade | C | Si | Mn | P | S | Cr | Cu | Ni |
|---|---|---|---|---|---|---|---|---|
| S355J0W | ≤0.16 | ≤0.50 | 0.50-1.50 | ≤0.030 | ≤0.025 | 0.30-1.25 | 0.25-0.55 | ≤0.65 |
S355J0W Mechanical Properties
| Thickness (mm) | Yield Strength (MPa) | Tensile Strength (MPa) | Elongation (%) |
|---|---|---|---|
| ≤16 | ≥355 | 470-630 | ≥22 |
| 16-40 | ≥345 | 470-630 | ≥22 |
| 40-63 | ≥335 | 470-630 | ≥22 |
| 63-80 | ≥325 | 470-630 | ≥22 |
| 80-100 | ≥315 | 470-630 | ≥21 |
Contact now to get S355J0W Corten Steel Quote
Impact Test Of S355J0W Corten Steel
| Grade | Impact Temperature | Minimum Impact Energy |
|---|---|---|
| S355J0W | 0°C | ≥27J |
Available Dimensions of S355J0W Corten Steel
| Item | Range |
|---|---|
| Thickness | 3mm – 150mm |
| Width | 1000mm – 3500mm |
| Length | 3000mm – 18000mm |
| Surface | Natural, Shot Blasted, Painted |
| Delivery Condition | Hot Rolled |

S355J0W Heavy Steel Plate has excellent mechanical properties and atmospheric corrosion resistance. Its chemical composition contains alloying elements that provide superior strength and toughness.
This steel plate is especially suitable for harsh environments such as marine engineering and bridge construction. With continuous investment in infrastructure projects, the demand for S355J0W Steel Plate is steadily increasing.
The application range of S355J0W Heavy Steel Plate is extensive. In addition to construction and bridges, it is widely used in the manufacturing of large equipment, cargo ships, and offshore oil platforms.
These industries require materials with high corrosion resistance and strength, and S355J0W Weathering Steel Plate can effectively meet these requirements. As these industries continue to develop, the market demand for S355J0W Steel Plate is expected to grow steadily.
With the increasing focus on environmental sustainability, more companies are paying attention to the long-term performance of construction materials.
Contact now to get a S355J0W Corten Steel Quote

S355J0W Corten Steel
Due to its excellent weather resistance, EN 10025-5 S355J0W Steel can reduce maintenance frequency and costs, providing good economic benefits during long-term use. This advantage encourages more companies to select S355J0W Steel Plate for their projects, further driving market demand.
In addition, the rapid development of the construction industry is another important factor contributing to the increasing demand for S355J0W Thick Steel Plate.
As urbanization accelerates, various construction projects continue to emerge, especially high-rise buildings and large public infrastructure projects. These projects require large quantities of thick steel plates as structural materials, making S355J0W Steel Plate an ideal choice.
The growth of international trade has also created new opportunities for the S355J0W Steel Supplier market. As globalization continues to expand, more companies are exploring overseas markets.
Equivalent Grades of S355J0W Corten Steel
| Standard | Equivalent Grade |
|---|---|
| ASTM | A588 Grade A |
| JIS | SPA-H |
| GB/T | Q355NH |
| COR-TEN | Corten A |
As a product that meets international standards, S355J0W Heavy Steel Plate has strong market competitiveness, especially in developing countries where infrastructure construction is growing rapidly, creating broader market opportunities for weather resistant steel products.
In future development trends, the demand for S355J0W Heavy Steel Plate is expected to continue growing. Especially in infrastructure construction, manufacturing, and international trade, S355J0W Steel Plate will continue to play an important role.
At the same time, companies should pay close attention to market changes and adjust their production strategies in a timely manner to adapt to evolving market demand.
S355J0W Steel Plate delivers outstanding weather resistance, high strength, and long-term durability for demanding structural projects.
Whether used in bridges, marine engineering, heavy equipment, or architectural structures, EN 10025-5 S355J0W Steel helps reduce maintenance costs while extending service life.
Choose a reliable S355J0W Steel Supplier to get stable quality, customized sizes, fast delivery, and competitive pricing for your next project.
Contact now to get a S355J0W Corten Steel Quote
What is S355J0W used for?
S355J0W weathering steel is widely used in bridges, railway wagons, shipping containers, building façades, landscape structures, outdoor sculptures, and general steel structures exposed to atmospheric conditions, especially in temperate and non-extreme cold regions.
What is the difference between S355J0W and S355J2W?
The main difference is low-temperature impact toughness. S355J0W is tested at 0°C, while S355J2W is tested at -20°C, meaning S355J2W performs better in colder climates. Their strength and corrosion resistance are otherwise very similar.
Does S355J0W steel rust?
Yes, but in a controlled way. S355J0W forms a dense protective rust layer (patina) on its surface, which prevents deeper corrosion. This makes it different from ordinary carbon steel, which continues to corrode without protection.
Does S355J0W need painting?
In most outdoor applications, S355J0W does not require painting. Its natural protective oxide layer reduces the need for coating and maintenance, which helps lower lifecycle costs.
Is S355J0W easy to weld?
Yes. S355J0W has good weldability using standard welding methods such as MAG and arc welding. In most cases, no complex post-weld heat treatment is required.
What environments is S355J0W suitable for?
S355J0W is suitable for temperate and subtropical climates, including urban outdoor structures, bridges, containers, and coastal or high-humidity environments where extreme low-temperature conditions are not present.
How long does S355J0W steel last?
When properly used in suitable environments, S355J0W weathering steel can significantly extend service life compared to normal carbon steel, often lasting several decades with minimal maintenance.