FE 510 C1K1 Steel Description
FE 510 C1K1 is a structural weathering steel which is also referred to as atmospheric corrosion resistant steel. The main alloying elements are chromium nickel and copper with added phosphorous which gives it excellent self protecting qualities.
As the steel reacts with elements in the atmosphere, the material forms a layer of rust over time which in essence protects the steel from corrosion.

FE 510 C1K1 steel is the Equivalent grades as S355J0WP (1.8945) steel in EN 10025 - 5 : 2004 standard and WR50A steel in BS 4360 standard and also E36WA3 steel in NFA 35-502 standard.
FE 510 C1K1 Steel Delivery state
Hot Rolled, Cold Rolled, Normalized, Quenched, Tempering, Thermal Mechanical Control Process (TMCP), Electroslag Remelting Technical, HIC test.
FE 510 C1K1 Steel Application
FE 510 C1K1 (which is an equivalent grade to Corten A) provides a long lasting and economic structural steel solution for use in applications such as steel bridges stack gas applications and in steel sculptured buildings due to the material's aesthetically pleasing finish.
Moreover, FE 510 C1K1 steel with improved atmospheric corrosion resistance has a wide range of applications: architecture, smokestacks, fabrication, freight wagons, silos, pylons etc.

FE 510 C1K1 Steel Chemical Composition
| C % | Mn % | Cr % | Si % | CEV % | S % |
| Max 0.12 | Max 1 | 0.3-1.25 | Max 0.75 | Max 0.52 | Max 0.035 |
| Cu % | P % | N % | |||
| 0.25-0.55 | 0.06 - 0.15 | Max 0.009 |
For long products the P and S content can be 0.005% higher.
The FE 510 C1K1 steels may show a Ni content of max. 0,65 %.
The max. value for nitrogen does not apply if the chemical composition shows a minimum total Al content of 0,020 % or if sufficient other N binding elements are present. The N binding elements shall be mentioned in the inspection
FE 510 C1K1 Steel Mechanical Properties
| Grade | Min. Yield Strength Mpa | Tensile Strength MPa | Impact | ||||||||
| FE 510 C1K1 | Nominal Thickness (mm) | Nominal Thickness (mm) | degree | J | |||||||
| Thick mm | ≤16 | >16 ≤40 |
>40 ≤63 |
>63 ≤80 |
>80 ≤100 |
>100 ≤150 |
≤3 | >3 ≤100 | >100 ≤150 | 0 | 27 |
| FE 510 C1K1 | 355 | 345 | …. | …. | …. | …. | 510-680 | 470-630 | …. | ||
The tensile test values given in the table apply to longitudinal samples; in case of strip and sheet steel of widths of ≥600 mm they apply to transverse samples.
If FE 510 C1K1 mechanical properties have been significantly modified by heavy coldforming, either stress relief annealing or normalised may be applied. Normalised should also be applied following hotforming outside of the temperature range of 750 - 1.050 °C and after overheating.
FE 510 C1K1 Steel Services
Cutting, Painting, shot blast, and The third party inspection in DNV, BV, LR, GL, ABS, CCS , SGS, and others in super thick ship steel plate.
Gnee Corten Steel is specialized in super thick atmospheric corrosion resistance of structural steel plate.Bebon International is a professional FE 510 C1K1 steel exporter and a steel Stockist in china.
We keep more than 1000 tons FE 510 C1K1 steel in stock every month. Besides that, Gnee Steel has very good relationship with every big steel mill, so we could promise the delivery time and the competitive price compared with other companies.
So, if you have any inquiry about FE 510 C1K1 steel, if you are looking for a sincerely FE 510 C1K1 steel supplier and want to get the FE 510 C1K1 steel price, please do not hesitate to contact us.
Any need in FE 510 C1K1 steel grade, please feel free to contact us by email or calling to us, we will supplier high quality FE 510 C1K1 steel with competitive price to you soon.