Fe 360 DK1 Steel Description
Fe 360 DK1 steel grade is a hot rolled products of structural steels in technical delivery conditions with improved atmospheric corrosion resistance.

Fe 360 DK1 steel is the Equivalent grades as S235J2W ( 1.8961 ) steel in EN 10025 - 5 : 2004 standard and WTSt 37-3 steel in SEW087 standard and also E24W4 steel in NFA 35-502 standard
Fe 360 DK1 Steel Delivery state
Hot Rolled, Cold Rolled, Normalized, Quenched, Tempering, Thermal Mechanical Control Process (TMCP), Electroslag Remelting Technical, HIC test.
Fe 360 DK1 Steel Application
Because of its low carbon content and fine-grained structure, Fe 360 DK1 Steels with improved atmospheric corrosion resistance have excellent weldability.So Fe 360 DK1 steel is mainly used for manufacturing welded,riveted or bolted structures.
Moreover, Fe 360 DK1 steel with improved atmospheric corrosion resistance has a wide range of applications: architecture, smokestacks, fabrication,freight wagons, silos, pylons and bridges.

Fe 360 DK1 Steel Chemical Composition
| C % | Mn % | Cr % | Si % | CEV % | S % |
| Max 0.13 | 0.2-0.6 | 0.4-0.8 | Max 0.4 | Max 0.44 | Max 0.3 |
| Cu % | P % | ||||
| 0.25-0.55 | Max 0.035 |
For long products the P and S content can be 0.005% higher
The Fe 360 DK1 steels may show a Ni content of max. 0,65 %
The Fe 360 DK1 steels shall contain at least one of the following elements: Al total ≥ 0,020 %, Nb: 0,015 - 0,060 %, V: 0,02 - 0,12 %, Ti: 0,02 - 0,10 %. If these elements are used in combination, at least one of them shall be present with the minimum content indicated.
Fe 360 DK1 Steel Mechanical properties
| Grade | Min. Yield Strength Mpa | Tensile Strength MPa | Impact | ||||||||
| Fe 360 DK1 | Nominal Thickness (mm) | Nominal Thickness (mm) | degree | J | |||||||
| Thick mm | ≤16 | >16 ≤40 |
>40 ≤63 |
>63 ≤80 |
>80 ≤100 |
>100 ≤150 |
≤3 | >3 ≤100 | >100 ≤150 | -20 | 27 |
| Fe 360 DK1 | 235 | 225 | 215 | 215 | 215 | 195 | 360-510 | 360-510 | 350-500 | ||
The tensile test values given in the table apply to longitudinal samples; in case of strip and sheet steel of widths of ≥600 mm they apply to transverse samples.
If Fe 360 DK1 mechanical properties have been significantly modified by heavy coldforming, either stress relief annealing or normalised may be applied. Normalised should also be applied following hotforming outside of the temperature range of 750 - 1.050 °C and after overheating.
Fe 360 DK1 Steel Services
Cutting, Painting, shot blast, and The third party inspection in DNV, BV, LR, GL, ABS, CCS , SGS, and others in super thick ship steel plate.
Gnee Steel is specialized in super thick atmospheric corrosion resistance of structural steel plate. Gnee is a professional Fe 360 DK1 steel exporter and a steel Stockist in china.
We keep more than 1000 tons Fe 360 DK1 steel in stock every month. So, if you have any inquiry about Fe 360 DK1 steel, if you are looking for a sincerely Fe 360 DK1 steel supplier and want to get the competitive Fe 360 DK1 steel price, please do not hesitate to contact us.
We will offer you the high quality steel,reasonable price and short leadtime.
Contact now to get Fe 360 DK1 Quote