S355J2G2W steel description
As a structural weathering steel, S355J2G2W steels have a super property. due to S355J2G2W steel chemical compositions, these steels exhibit increased resistance to atmospheric corrosion compared to other steels.

This is because the S355J2G2W steel forms a protective layer on its surface under the influence of the weather.
S355J2G2W steel deliver condition
Hot Rolled, Cold Rolled, Normalized, Quenched, Tempering, Thermal Mechanical Control Process (TMCP), Electroslag Remelting Technical, HIC test.
S355J2G2W steel application range
S355J2G2W steel weathering steel has a widely use in Mine fans, earth moving buckets, trailers and large road vehicles, drill rings, cranes, excavators, underground mining equipment, bridges and other high strength components requiring superior toughness.

S355J2G2W steel chemical composition(%)
| C | Si | Mn | P | S | Cu | Cr | Ni | V | Nb | Al |
| Max 0.16 | Max 0.50 |
Max 0.50-1.50 |
Max 0.035 |
Max 0.035 |
Max 0.25-0.55 |
Max 0.40-0.80 |
Max 0.65 |
Max 0.02-0.12 |
Max 0.015-0.060 |
Min 0.02 |
S355J2G2W steel mechanical property
| Thickness | Yield Strength ReH[N/mm2] transv.min |
Tensile Strength Rm[N/mm2]transv |
Fracture Elongation[%]transv. min. | Notch Impact Energy1)Ch Vcomplete samplelongitud. min [J] |
| ---- | 355 | 510-610 | 22 | ---- |
Contact now to get S355J2G2W Quote
About Us
Gnee Group was established in 2008 and is a steel manufacturing company specialized in weathering steel raw materials and fabricated components.
We supply a wide range of standard-grade Corten steel materials and undertake the production of customized weathering steel parts and complete project solutions.
If you would like to learn more about weathering steel or are interested in making a purchase, please send an email to corten@gneesteelgroup.com. We will get back to you as soon as we receive your message.