EN 10025-5 S355J2WP Weathering Steel Plate: Grades and Properties

Sep 04, 2025 Leave a message

What S355J2WP Steel Plate Is

S355J2WP is a hot rolled structural steel plate supplied under EN 10025-5, the part of the European structural steel series that covers steels with improved atmospheric corrosion resistance. The designation carries three pieces of information: S for structural steel, 355 for the minimum yield strength in MPa at the thinnest section, and J2 for an impact energy of 27 J tested at minus 20 degrees Celsius. The final P marks the phosphorus-bearing variant, in which a deliberately higher phosphorus range is used to strengthen the protective oxide layer.

The alloying concept is straightforward. Copper, chromium and nickel are added together with phosphorus, and the combination allows a firmly adhering rust layer to form on the surface rather than flaking away. As the steel reacts with oxygen and moisture, that layer gradually becomes a barrier that slows further attack, which is why the material can be left unpainted in many outdoor and industrial environments and still deliver a long service life with an attractive brown surface.

Delivery States and Plate Availability

EN 10025-5 fixes the property requirements but not a single production route, so S355J2WP plate is supplied in a range of conditions depending on thickness and on the fabricator's needs:

As-rolled or hot rolled, the normal condition for general structural plate

Normalised, used when a uniform ferrite-pearlite structure is wanted or after hot forming above the recommended temperature window

Thermo-mechanically controlled processed, for improved toughness at heavier thicknesses

Quenched and tempered, or stress relief annealed after severe cold forming, where the application demands it

Cold rolled for thinner sheet applications such as container panels

With additional testing such as hydrogen induced cracking evaluation when the plate is destined for wet sour service

Because phosphorus raises the risk of segregation and lowers toughness in heavy sections, the phosphorus-bearing grades are usually chosen for thinner plate and for structures where welding is limited or carefully controlled. Heavier welded structures normally move to the low-phosphorus S355J2W instead.

Chemical Composition

Typical heat analysis limits for S355J2WP are given below. Where long products are supplied, the phosphorus and sulfur limits may be relaxed slightly, and small amounts of nitrogen-binding elements such as aluminium, niobium, vanadium or titanium are added to control grain size.

Element Requirement (%) Comment
Carbon 0.12 max Kept low for toughness and weldability
Silicon 0.75 max Deoxidation
Manganese 1.00 max Strength and deoxidation
Phosphorus 0.06 - 0.15 Deliberately high to improve corrosion resistance
Sulfur 0.035 max Inclusion control
Copper 0.25 - 0.55 Main patina forming element
Chromium 0.30 - 1.25 Stabilises the oxide layer
Nickel 0.65 max Optional addition, tolerances apply
Carbon equivalent (CEV) 0.52 max Weldability control, carbon plus alloying contributions

At least one grain refining element must be present at or above its minimum content - total aluminium 0.020 percent, or niobium 0.015 to 0.060 percent, or vanadium 0.02 to 0.12 percent, or titanium 0.02 to 0.10 percent. If several are used together, at least one must still meet its individual minimum.

Mechanical Properties

Strength values fall as section thickness rises, because the cooling rate after rolling is slower in heavy plate. The table below shows the minimum yield strength and the tensile range normally certified for S355J2WP.

Thickness range (mm) Minimum yield strength (MPa) Tensile strength (MPa)
Up to 3 355 510 - 680
Over 3 to 100 355 down to 315 by sub-range 470 - 630
Over 100 to 150 295 450 - 600

Impact testing is carried out on Charpy V-notch longitudinal specimens at minus 20 degrees Celsius with a minimum absorbed energy of 27 J, which is what the J2 quality class guarantees. The tensile test values above apply to longitudinal samples; for strip and sheet at least 600 mm wide, transverse samples are used instead. If properties have been altered by heavy cold forming, either stress relief annealing or normalising may be applied, and normalising is also recommended after hot forming outside the 750 to 1050 degree Celsius window or after overheating.

Applications, Welding and Fabrication Notes

Under EN 10025-5, S355J2WP plate is used where a combination of load carrying capacity and long term atmospheric durability is required, most notably:

Container and freight wagon steelwork, the traditional application for the phosphorus-bearing grade

Architectural cladding, facades and exposed columns where the weathered surface is a design feature

Smokestacks, chimneys, silos and hoppers in industrial plant

Pylons, transmission masts and lighting columns

Bridge components and highway structures in moderately corrosive atmospheres

Fabrication follows normal structural steel practice with two cautions. The higher phosphorus content makes the steel more sensitive to cracking in the heat affected zone, so low-hydrogen consumables, controlled heat input and qualified procedures are essential; the plate should not be substituted for the low-phosphorus J2W variant without checking the welding procedure. Forming and flame cutting are otherwise routine, and the cut edges will weather in the same way as the rolled surface once exposed.

Frequently Asked Questions

Q: What does the P in S355J2WP stand for?
It marks the phosphorus-bearing variant of the grade. The chemistry deliberately retains 0.06 to 0.15 percent phosphorus, which raises atmospheric corrosion resistance but also makes the steel more sensitive to welding, so the grade is normally used in thinner sections.

Q: How does S355J2WP differ from S355J2W?
The two grades share the same strength class and the same minus 20 degrees Celsius impact requirement. The difference is phosphorus: S355J2W keeps it low for better weldability and heavy section toughness, while S355J2WP trades some of that for a stronger protective oxide layer.

Q: Is EN 10155 still valid for this plate?
EN 10155 was the earlier weathering steel standard and has been replaced by EN 10025-5. Old drawings that reference EN 10155 with an S355J2WP designation are normally satisfied by plate to EN 10025-5, but the acceptance should name the edition in use.

Q: Can S355J2WP be used without paint?
Yes, in the right environment. Bare use depends on regular wet and dry cycling so the patina can stabilise. Permanently damp, buried or chloride-heavy conditions prevent that layer from forming and call for a coating system instead.

Q: What thicknesses and widths are available?
Plate is commonly rolled from about 3 mm to 150 mm, with widths up to roughly 4 metres and lengths up to 12 metres depending on the mill. Thickness determines which yield strength sub-range applies, so it should always be stated on the order.

Q: Does the plate need extra testing?
Beyond the standard tensile and impact tests, additional options such as ultrasonic examination, third party witnessing or corrosion testing can be arranged when the application or the purchaser's specification requires them.