What is the specification of A588 Gr.C structural steel sheet

Nov 13, 2025 Leave a message

ASTM A588 Grade C steel plate is a high-strength, low-alloy structural steel designed for excellent atmospheric corrosion resistance. It is widely used in structural and outdoor applications where long-term durability and reduced maintenance are required.

 

info-454-454

 

Chemical Composition

Element C Mn P S Si Ni Cr Mo Cu V Nb
Range 0.12–0.20% 0.60–1.00% ≤0.035% ≤0.04% 0.15–0.35% 0.40–1.00% 0.40–0.65% 0.08–0.15% 0.20–0.40% 0.05–0.10% 0.02–0.06%

 

Mechanical Properties

Property Value
Tensile Strength 585–700 MPa
Yield Strength ≥345 MPa
Elongation

≥21%

 

Industry News & Market Insight

As of mid-March, major national iron and steel enterprises produced an average daily crude steel output of 176.17 million tons, a 3.94% increase over the previous period. This represents approximately 5.29 billion tons of annualized production.

 

ASTM A588 Grade C steel plate stock inventory reached 14,203,900 tons, up 0.54% over the previous ten days, reflecting stable supply levels to meet growing infrastructure demands.

 

According to Citi analysts (April 5), the construction of Xiong'an New District is projected to significantly boost steel demand. The project may require 12–14 million tons of ASTM A588 Grade C steel annually, totaling 120–140 million tons over ten years, enough to build approximately 10,000 km of steel-framed bridges or 15,000 high-rise buildings.

 

The average service life of ASTM A588 Grade C steel in outdoor environments can reach 50 years or more due to its self-protecting corrosion-resistant layer, minimizing maintenance costs over the project lifespan.

 

Applications & Advantages

Structural Projects: Bridges, buildings, heavy-duty frameworks requiring high strength (585–700 MPa) and yield strength ≥345 MPa, capable of supporting large-scale structural loads exceeding 50 tons per beam.

 

Outdoor & Architectural Use: Retaining walls, facades, and infrastructure exposed to harsh weather. ASTM A588 Grade C steel can resist corrosion in marine and industrial environments with annual material loss <0.02 mm.

 

Cost Efficiency: The self-protecting rust layer eliminates the need for painting, reducing maintenance costs by up to 30–40% over conventional carbon steel.

 

Long-Term Durability: Excellent resistance to atmospheric corrosion ensures structural integrity for decades, even under high humidity, coastal, or industrial conditions.

 

Premium Quality and Service

We provide first-class ASTM A588 Grade C steel plates with guaranteed quality and full technical support. Contact us anytime for inquiries or orders.

 