Classification Of Laser Cutting Weathering Steel Plates

Jun 18, 2025 Leave a message

Laser cutting can be divided into four categories: laser vaporization cutting, laser melting cutting, laser oxygen cutting, laser scribing and controlled cracking.

1) Laser vaporization cutting

A high energy density laser beam is used to heat the workpiece, causing the temperature to rise rapidly and reach the boiling point of the weathering plate in a very short time, and the material begins to vaporize to form steam. The jet speed of these vapors is very large. When the vapors are ejected together, they form a blockage on the material. The vaporization heat of the material is usually very large, so laser vaporization requires a lot of power and power density.

Laser vaporization cuts are generally used to cut extremely thin metal materials and non-metallic materials (such as paper, cloth, wood, plastic and rubber, etc.).

2) Laser melting and cutting

When laser cutting is performed, the metal material is melted by laser heating, and then a non-oxidizing gas (Ar, He, N, etc.) is ejected through a nozzle coaxial with the beam, and then a blockage is formed according to the strong pressure of the gas. Laser melting and cutting does not require complete evaporation of the metal, and the energy required is only 1/10 of evaporation and cutting.

Laser melting cutting is mainly used to cut materials that are not easy to oxidize or active metals, such as stainless steel, titanium, aluminum and their alloys.

3) Laser oxygen cutting

The principle of laser oxygen cutting is similar to oxyacetylene cutting. It uses laser as a preheating heat source and uses active gas such as oxygen as cutting gas. On the one hand, the blown gas interacts with the cut metal, causing an oxidation reaction and emitting a large amount of oxidation heat. On the other hand, the molten oxide and melt are blown out of the reaction zone to form a block in the metal. Since the oxidation reaction during the cutting process generates a lot of heat, the energy required for laser oxygen cutting is only 1/2 of that for fusion cutting, and the cutting speed is much faster than laser vaporization cutting and fusion cutting. Laser oxygen cutting is mainly used for easily oxidized metal materials such as carbon steel, titanium steel and heat-treated steel.

4) Laser scribing and crack control

Laser scribing is the use of high energy density laser to scan the surface of brittle materials, so that the material is heated and vaporized to emit small grooves, and then a certain pressure is applied, and the brittle material will break along the small grooves. The lasers used for laser scribing are usually Q-switched lasers and CO2 lasers.

Controlled cracking refers to the steep temperature distribution that occurs when laser grooves weathering steel, which will produce some thermal stress in the brittle material, causing the material to break along the small grooves.