The core material of weathering steel pipes is low alloy steel. By adding copper (0.2%~0.5%), phosphorus (0.07%~0.15%), chromium (0.5%~1.25%) and other elements, a dense oxide layer is formed to prevent the spread of rust. According to the national standard GB/T 4171-2008, typical grades include 09CuPCrNi-A (tensile strength ≥470MPa) and SPA-H (Japanese standard JIS G3125), and its atmospheric corrosion resistance is 2~8 times that of ordinary carbon steel (data source: Technical report of China Iron and Steel Association). This type of steel pipe is often used in outdoor scenes such as bridges and containers.
Note: Weathering steel pipe ≠ stainless. A uniform rust layer will form on its surface, but the interior will no longer continue to corrode, which is essentially different from traditional stainless steel (containing more than 12% chromium).