ASTM A423 Corten Steel Pipe

ASTM A423 Corten Steel Pipe

Products Description ASTM A423 Cortenn Steel Pipe is a low alloy carbon steel grade that forms an oxide layer on the surface when exposed to extreme weather conditions. This layer is called patina and it work as a protective coating on ASTM A423 products, resisting corrosion for a longer period....
Send Inquiry
Description
Technical Parameters
 

Products Description

 

ASTM A423 Cortenn Steel Pipe is a low alloy carbon steel grade that forms an oxide layer on the surface when exposed to extreme weather conditions. This layer is called patina and it work as a protective coating on ASTM A423 products, resisting corrosion for a longer period.

 

product-553-552

 

They can be found in complex piping due to their ease of fixture and corrosion resisting properties.

 

 

Specification

 

Size Range ½” OD to 16” OD
Standards AASTM A 423 / ASME SA 423
Grade ASTM A423 GR 1 / ASME SA423 GR 1
Type Round, Square, Rectangle, Hydraulic, Honed Tubes
Length Single Random, Double Random & Customize Size
Type Weathering Steel
End

Plain End, Beveled End, Threaded End

 

 

Mechanical Properties of ASTM A423 Corten Steel Grade 1 Pipes & Tubes

 

Grade Yield Strength MPa(min) Tensile Strength MPa Elongation % (min)
Corten A 355 470-630 20

 

 

Chemical Compositions of ASTM A423 Corten Steel Grade 1 Pipes & Tubes

 

Element C, % Mn, % P, % S, % Si, % Cu, % Cr, % Ni, %
A/SA 423 GR 1
 
0.15 max. 0.55 max. 0.06–0.16 0.060 max. 0.10 min. 0.20–0.60 0.24–1.31 0.20–0.70

 

 

Manufacture Process

 

 

Seamless

ERW (electric resistance welded)

 

 

Heat Treatment

 

Normalized or otherwise heat treated

 

 

Size range of ASTM A423 tube

 

Outside Nominal Wall Inside Weight
Diameter Pipe Diameter Thickness Diameter Lbs
Inches Inches Inches Inches Per Foot
1.660 1-1/4 .140 1.380 2.273
1.315 1 .133 1.049 1.679
1.900 1-1/2 .145 1.610 2.718
2.875 2-1/2 .203 2.469 5.793
2.375 2 .154 2.067 3.653
6.625 6 .28 6.056 18.97
3.50 3 .216 3.068 7.576
4.50 4 .237 4.026 10.79
4 3-1/2 .226 3.548 9.109
5.563 5 .258 5.047 14.62
8.625 8 .322 7.981 28.55

 

 

Corten Steel A423 Pipes & Tubes Application

 

Petrochemical Oil & Gas Air Preheater Unit Refineries Nuclear Power
Power Plant Fossil Fuel Plants Breweries Chemical Steam Generating Boiler

 

Cement Water Supply Systems Steel Plant Mills Engineering Co.
Shipbuilding Heat Exchangers Architectural Construction Cogeneration Facilities Economiser

 

Corten Steel A423 Pipes

 

Hot Tags: ASTM A423 Corten Steel Pipe, China ASTM A423 Corten Steel Pipe manufacturers, suppliers, Rectangular Corten Steel Tubes, Sulfuric acid dew point Seamless pipe, Sulfuric Acid Resistant pipe, Welded Corten Steel Pipe, 09CrCuSb Corten Pipe, Round corten Pipe