Products Description
S355J0WP weather resistant steel plate is a structural weathering steel, also known as atmospheric corrosion-resistant steel. Its primary alloying elements are chromium, nickel, and copper, with phosphorus added to impart exceptional self-protection properties.
When the steel reacts with atmospheric elements, a dense, stable rust layer forms on the surface over time, effectively preventing further corrosion.
Regarding mechanical properties, the yield strength of S355J0WP hot rolled weather resistant steel plate varies with thickness: no less than 355 MPa for thicknesses up to 16 mm, 345 MPa for 16–40 mm, and 335 MPa for 40–63 mm. Its tensile strength ranges from 470 to 630 MPa, with elongation exceeding 20%.
It can withstand an impact of 27 joules at 0°C, ensuring excellent toughness and reliability.
Chemically, the steel contains 0.40–0.80% chromium, 0.25–0.55% copper, nickel not exceeding 0.65%, and phosphorus between 0.035–0.12%. These elements collectively impart exceptional weather resistance to the material.
S355J0WP high stregth weather resistant steel plate offers not only outstanding strength and corrosion resistance but also an aesthetically pleasing surface finish.
This makes it a durable and economical solution for architectural applications such as steel bridges, chimney exhaust systems, exterior cladding, and steel sculptures.

Chemical composition of EN 10025-5 S355J0WP steel plate
|
Grade |
C max |
Si max |
Mn |
P max |
S max |
Cr |
Cu |
|
S355J0WP |
0.13 |
0.40 |
0.20-0.60 |
0.035 |
0.030 |
0.40-0.80 |
0.25-0.55 |
Mechanical property of EN 10025-5 S355J0WP steel plate
|
Tensile Strength (MPa) |
Yield Strength (MPa) |
% Elongation in 2 in. (50mm) min |
Impacting Test Temperature (°C) |
|
510 |
355 |
19 |
0 |
Equivalent grades of EN S355J0WP corten steel plate weather resistant steel sheet
| EU | USA | Germany | Japan | France | England | European old | Italy | China | Poland | Czechia | Inter |
| EN | - | DIN,WNr | JIS | AFNOR | BS | EN | UNI | GB | PN | CSN | ISO |
| S355J0WP | Gr.1 | 9CrNiCuP324 | SPA-H | E36WA3 | WR50A | Fe510C1KI | Fe510C1K1 | 09CuPCrNi-A | 10H | 15217 | Fe355W-1A |
| WR50B | S355JOWP | ||||||||||
| WR50C |
Application
S355J0WP corten steel plate offers a durable and economical structural steel solution for steel bridges, chimney gas applications, and steel sculpture architecture, thanks to its aesthetically pleasing surface finish.
Furthermore, this steel with enhanced atmospheric corrosion resistance has a wide range of applications: covering building structures, chimneys, metal products, freight cars, silos, towers, and more.
Its suitability for these applications stems from their prolonged exposure to harsh environments like wind, rain, humidity, salt spray, or flue gases.
While ordinary steel rapidly corrodes and loses strength under such conditions, S355J0WP high strength low alloy corten steel plate develops a dense, stable protective rust layer on its surface.
This layer effectively resists corrosion, extends service life, and reduces frequent maintenance costs. Simultaneously, it delivers a distinctive natural aesthetic appeal in architectural and landscape applications.
Contact now to get S355J0WP Quote
S355JOWP steel sheet is a top grade in the weathering steel family. It is essential for projects that need both structural strength and a unique, self-protecting look.

People commonly know this steel by the trademark Corten, and it forms a stable, rust-like layer when exposed to air, which means you don't need to paint it and can reduce long-term care costs.
Its uses range from famous building fronts and bridges to industrial containers and rail cars.
Shipping Terms
Delivery Time:
Stock Items: Within 7–10 business days
Custom Orders: 15–30 days (depending on quantity and specifications)
Shipping Methods: Ocean freight, rail, road, air freight (selected based on customer requirements and destination)
Packaging: Steel strapping, waterproof tarpaulin covering, with wooden pallets or custom packaging provided when necessary
Shipping Ports: Tianjin, Qingdao, Shanghai, Lianyungang, and other major ports
Insurance & Services: CIF terms (including insurance) available; third-party inspection supported (SGS, BV, CE, etc.)
Customs Clearance Documents: Bill of Lading, Commercial Invoice, Packing List, Certificate of Origin, Material Test Certificate (MTC)

Hot Tags: en 10025-5 s355j0wp weather resistant steel plate, China en 10025-5 s355j0wp weather resistant steel plate manufacturers, suppliers, High durability steel coil, Anti Rust Steel plate, Hot weathering steel Plate, Cold Rolled Sheet, perforated corten steel facade, Corten B