High Strength Low Alloy S235J0W Corten Steel Plate

High Strength Low Alloy S235J0W Corten Steel Plate

Steel Grade: S235J0W High Strength Corten Steel Plate
Steel Standard: EN 10025-5
Thickness: mm-450mm
Width: 1000mm-4200mm
Length: 3000mm-18000mm
S235J0W steel surface treatment: Shot blasting and painting or coated.
Send Inquiry
Description
Technical Parameters

Products Description

 

S235J0W Corten Steel Plate, due to its excellent atmospheric corrosion resistance, is primarily used in harsh climatic environments characterized by humidity, heavy rainfall, salt spray, strong winds and sandstorms, or significant temperature fluctuations.

S235J0W Corten Steel

Its minimum yield strength is 235 MPa, and for plates with a thickness less than 100 mm, the tensile strength should range between 360 and 510 MPa.

 

specification

 

S235J0W Plate

Steel Grade: S235J0W High Strength Corten Steel Plate

 


Steel Standard: EN 10025-5

 


Thickness: mm-450mm

 


Width: 1000mm-4200mm

 


Length: 3000mm-18000mm

 

 

S235J0W steel surface treatment: Shot blasting and painting or coated.

 

mechanical properties of grade S235J0W

 

Minimum yield strength Reh
MPa

Tensile strength Rm
MPa

Minimum elongation - A
Lo = 80 mm

Minimum elongation - A
Lo = 5,65 * √So (%)

Steel grade

Nominal thickness
mm

Nominal thickness
mm

Nominal thickness
mm

 

≤16

>16
≤40

>40
≤63

>63
≤80

>80
≤100

>100
≤150

≤3

>3
≤100

>100
≤150

>1,5 ≤2

>2
≤2,5

>2,5
≤3

>3
≤40

>40
≤63

>63
≤100

>100
≤150

 
S235J0W

235

225

215

215

215

195

360-510

360-510

350-500

19

20

21

26

25

24

22

 

chemical composition of grade S235J0W

 

Steel grade

C
max.
%

Si
max.
%

Mn
%

P
max.
%

S
max.
%

N
max.
%

Cu
%

Cr
%

CEV
max. %

 
S235J0W

0,13

0,40

0,20 - 0,60

0,035

0,035

0,009

0,25 - 0,55

0,4 - 0,8

0,44

 

Notch impact test

 

Temperature
°C

-20

0

 

Min. absorbed energy
J

27

27

 

Application

 

S235J0W Weathering Steel Plate, the steel is especially intended for use in heavily loaded parts of welded structures such as, bridges, flood gates, storage tanks, water supply tanks, etc., for service at ambient and low temperatures.

Corten Application

Transportation and Delivery

 

We understand the critical importance of safe steel plate transportation for our customers.

 

Timely Delivery: Standard orders ship within 7–15 business days after receiving advance payment.

 

Multiple Shipping Methods: Choose from ocean freight, land transport, rail, or air shipping to meet your needs, ensuring fast and secure delivery.

 

Professional Packaging: Products are secured with steel strapping, covered with waterproof tarps, and reinforced on wooden pallets to effectively prevent moisture, impact, and deformation during transit.

 

Flexible Shipping Origins: We support shipments from major ports including Shanghai, Tianjin, Qingdao, and beyond, covering global destinations.

 

Contact now to get S235J0W Quote

 

About Us

 

Over the past decade, Gnee has continuously improved its supply chain management and R&D platforms.

The company introduced automation equipment and information management tools, achieving full-process digital control from procurement, production, quality inspection to logistics.

 

For years, Gnee has formed strategic partnerships with leading steel mills and manufacturers at home and abroad to enhance product competitiveness.

 

In 2022, Gnee accelerated the deployment of smart factories to improve production efficiency and quality continuously.,

 

The corporate culture has crystallized around core values: professionalism, integrity, innovation, and win-win cooperation.

Gnee Steel

Hot Tags: high strength low alloy s235j0w corten steel plate, China high strength low alloy s235j0w corten steel plate manufacturers, suppliers, ASTM Corten Plate, corten sheet, corten A steel, A588 steel sheet, Laser Cut Corten Steel Sheet, Corten A Steel Coil