S355J0W High Strength Low Alloy Weathering Steel Plate

S355J0W High Strength Low Alloy Weathering Steel Plate

S355J0W is a low-alloy high-strength structural steel, which belongs to the weathering steel under the European standard (EN 10025-5:2004), also known as atmospheric corrosion resistant steel.
Send Inquiry
Description
Technical Parameters

Products Description

 

S355J0W High Strength Low Alloy Weathering Steel Plate, which belongs to the weathering steel under the European standard (EN 10025-5:2004), also known as atmospheric corrosion resistant steel.

 

S355J0W High Strength Low Alloy Weathering Steel Plate

 

This kind of steel adds a small amount of corrosion resistant elements such as copper and nickel on the basis of ordinary steel to improve its corrosion resistance in atmospheric environment.

 

Specification

 

Standard EN 10025-5
Grade S355J0W, S355J0W+N
Category Atmospheric resistant steel, weathering steel
Thickness 1.2-150mm
Width 1220-4200mm
Length 5000-18000mm, or cut shapes as required
Form Plates, sheets,coils, Plain Sheet, flat steel, section steel, H beams, bars, Perforated Sheet, Chequered Plate
Finish Hot rolled plate (HR), Cold rolled sheet (CR)
Hardness Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.
Grade Corten Steel EN 10025 S355J0W+N

 

Features

 

product-526-527Exceptional weather resistance and corrosion resistance: S355J0W steel plates maintains long-term stable performance in outdoor environments without requiring additional coatings or anti-corrosion treatments, significantly reducing maintenance costs.

 

Its atmospheric corrosion resistance is 2–8 times that of ordinary carbon steel, and it can still form a dense, stable protective rust layer in humid, rainy, or industrially polluted atmospheres.

 

High Strength Characteristics: The minimum yield strength of this steel is no less than 355 MPa for thickness ≤16 mm, 345 MPa for 16–40 mm, and 335 MPa for 40–63 mm.

 

Its tensile strength ranges from 470–630 MPa, meeting diverse complex engineering requirements.

 

Excellent weldability and workability: S355J0W hot rolled steel sheet facilitates easy cutting, bending, welding, and other processing operations during manufacturing.

 

With an elongation of no less than 20%, it offers greater design flexibility for engineers and manufacturers.

 

Superior impact toughness: In 0°C impact tests, S355J0W Weather Resistant Steel Plates delivers impact energy of no less than 31 J, demonstrating excellent impact resistance and withstanding significant impact loads even in low-temperature environments.

 

Energy-saving and consumption-reducing advantages: Leveraging its superior weather resistance and strength properties, S355J0W reduces protective coating and maintenance costs by approximately 25–30%. Additionally, it enables 10–20% thinner steel sections in structural designs, effectively lowering material consumption while conserving labor and energy resources. This results in more competitive overall project costs.

 

Mechanical Properties of S355JOW

 

Grade Min. Yield Strength ReH MPa           Tensile Strength Rm MPa    
  Nominal Thickness (mm)           Nominal Thickness (mm)    
  <16 >16 <40 >40 <63 >63 <80 >80 <100 >100 <150 >3 >3 <100 >100 <150
S355JOW 355 345 335 325 315 295 510/680 470/630 450/600

 

Chemical Composition of S355JOW

 

  %
C 0.16
Si 0.50
Mn 0.50/1.50
P 0.035
S 0.035
N 0.009
Cr 0.40/0.80
Cu 0.25/0.55

 

Equivalent grades of grade S355J0W

 

UNI

EU 155

France

NFA35-502

Germany

WBL 087

U.K.

BS 4360

Japan

JIS G3114

USA

ASTM

Fe510 C2K1

E 36WB 3

 

WR50B

SMA 50AW

A588 Gr. A

 

application

 

S355J0W steel plates is suitable for various welded, bolted, and riveted structures, such as steel frame structures, bridges, storage tanks and vessels, exhaust systems, vehicles, and equipment construction.

 

Corten Steel Facade

additional service

 

Cutting(NC Cutting), painting, shot blast, welding, galvanization

 

Trade Terms: FOB, CFR, CIF

 

Payment Terms: T/T, L/C at sight

 

 

Contact now to get S355J0W Quote

 

about Us

 

At Gnee, product safety is at the heart of everything we do. From raw materials to finished goods, we ensure every step in the production chain meets rigorous international safety standards.

Our Safety-Related Certifications Include:

 

ISO 45001:2018 Occupational Health & Safety Management
Guarantees a safe working environment in compliance with global safety practices.

 

EN 1090 + A1 CE Certification for Structural Steel
Ensures mechanical integrity and safety for demanding structural applications in the EU.

 

SGS / TUV / BV Mechanical Property Test Reports
Verifies yield strength, tensile strength, and impact resistance according to global safety norms.

 

MSDS (Material Safety Data Sheet) - Available upon request
Offers safety guidance for handling, transport, and storage of our steel products.

 

Gnee is committed to more than just high-performance steel - we deliver safe and dependable solutions for every project.

 

product-800-1000

 