Products Description
Under GB/T 4171,there are weathering steel grade 09CuPCrNi-A steel plate,09CuPCrNi-B steel plate and 09CuP steel plate.Among these three different weathering steel grades,09CuPCrNi-B is limited in Phosphorus contains comparing with corten A steel plate and 09CuPCrNi-A steel plate.

09CuPCrNi-B Weather resistant steel plate Specification
Thickness: 2mm-450mm
Width:1000mm-4200mm
Length:3000mm-18000mm
Mechnical property for 09CuPCrNi-B corten plate
| Yield strength (Mpa) Min. | Tensile strength (Mpa) Min. | Elongation in ≥,% |
| 294 | 431 | 24 |
Chemical composition for 09CuPCrNi-B corten plate (Heat Analysis Max%)
| Main chemical elements composition of 09CuPCrNi-B | |||||||
| C | Si | Mn | P | S | Cu | Ni | Cr |
| 0.12 | 0.10-0.40 | 0.20-0.50 | 0.07-0.12 | 0.040 | 0.25-0.45 | 0.25-0.50 | 0.30-0.65 |
Application fields of 09CuPCrNi-B atmospheric steel
Construction field: 09CuPCrNi-B corten weathering steel can be used to manufacture bridges, building exterior walls, roofs, etc.
Vehicle manufacturing: 09CuPCrNi-B weathering steel can be used to manufacture structural parts for vehicles such as cars, trains, and ships.
Petroleum industry: 09CuPCrNi-B corten metal sheet can be used to manufacture oil pipelines, storage tanks and other equipment.
Other Terms
Packaging Details: Standard export seaworthy packing or as required.
Delivery Time: 30-50 days, 7 days for stock goods.
Loading Port: Shanghai ,Tianjin, Qingdao.
Offer Ability:5 000MT/Per Month.
MOQ: 1 Pcs.