09CuPCrNi-B Weather Resistant Steel Plate

Sep 30, 2025 Leave a message

09CuPCrNi-B steel plate is a kind of weather steel plate, and 09CuPCrNi-B steel has added phosphorous which makes the material best suited for gas flue applications and for aesthetic facias .

09CuPCrNi-B steel plate

09CuPCrNi-B steel plate specification

 

Steel Grade: 09CuPCrNi-B Steel Standard: GB4171-84
Thickness: 2mm-450mm, Width:1000mm-4200mm, Length:3000mm-18000mm

 

09CuPCrNi-B Chemical composition

Grade

The Element Max (%)

 

09CuPCrNi-B

C

Si

Mn

P

S

≤0.12

0.10-0.40

0.20-0.50

0.06-0.12

≤0.020

Cr

Cu

Ni

RE

 

0.30-0.65

0.25-0.45

0.25-0.50

 

 

Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%

 

Grade

Thickness

Yield

Tensile

Elongation

Delivery state

09CuPCrNi-B

mm

Min Mpa

Mpa

Min %

 

4<

295

431

24

Hot rolling

≤4

265

402

27

Cold rolling

 

09CuPCrNi-B steel plate surface treatment: Shot blasting and painting or coated.

 

09CuPCrNi-B steel plate application
09CuPCrNi-B steel plate is used for shipping containers,steel bridges,vessels and tanks for preventing atmospheric corrosion usage.